Basic thin coated AC/DC electrode providing excellent mechanical properties. This electrode ensures fully penetrated root passes, even in adverse conditions. Low moisture content of the coating has a high resistance to moisture re-absorption. For vertical up applications.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded iso
150 J (111 ft-lb) -45 degC (-49 degF)
140 J (104 ft-lb) -50 degC (-58 degF)

Typical Tensile Properties

ConditionElongationShielding GasTensile Strength Yield Strength
As Welded30 %ISO550 MPa (80 ksi)470 MPa (68 ksi)

Deposition Data

Current Deposition Rate @ 90% I max Diameter Deposition Efficiency (%) Number of electrodes/kg weld metal Voltage
80-140 A 53 sec 1.3 kg/h (2,9 lb/h) 3.2 x 350.0 mm (1/8 x 13,8 in.) 61 % 52.0 22 V
110-180 A 62 sec 1.7 kg/h (3,7 lb/h) 4.0 x 350.0 mm (5/32 x 13,8 in.) 64 % 34.0 22 V

Classifications

Classifications SFA/AWS A5.1 : E7016-1 H4 R
EN ISO 2560-A : E 42 5 B 1 2 H5

Consumable Characteristics

Alloy Type Carbon manganese
Coating Type Basic covering
Diffusible Hydrogen < 4.0 ml/100 g
Welding Current AC, DC+(-)

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn Si
0.06 % 1.25 % 0.50 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Pipeweld 7016
5P753230G0 FIND A DISTRIBUTOR
5P754030G0 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..