Atom Arc 7018-SR
Atom Arc 7018-SR is an all-position low hydrogen electrode. The moisture resistance and welder appeal is similar to other Atom Arc electrodes. Atom Arc 7018-SR was developed to maintain 70 ksi (483 MPa) tensile strength after 16 hours stress relieving.
Industries
- Civil Construction
- Industrial and General Fabrication
- Mobile Equipment
- Power Generation
Welding Process
- SMAW/MMA (Stick)
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Mn | Mo | P | S | Si | |||||||||
0.06 % | 1.30 % | 0.10 % | 0.014 % | 0.014 % | 0.30 % | |||||||||
0.10 % | 0.30 % |