Atom Arc 7018 Acclaim

ESAB

Atom Arc 7018 Acclaim

The following items have been added to your list


x

Atom Arc 7018 Acclaim offers softer arc and excellent mechanical properties compared to the original Atom Arc 7018. Results include greater puddle control for ease of use in out-of-position welding applications and superior arc initiation desired by many newer welders. Both novice and seasoned welders can appreciate its excellent weld performance, wide operating range and easy clean up. Greater puddle control resulting in easier out-of-position welds, superior arc initiation and ease of use with wider operating range and minimal clean-up

BUY NOW


Industries

  • Automotive
  • Bridge Construction
  • Civil Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Railcars
  • Ship/Barge Building

Welding Process

  • SMAW/MMA (Stick)

Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded
115 J (85 ft-lb) -45 degC (-50 degF)
230 J (170 ft-lb) 29 degC (-20 degF)

Typical Tensile Properties

Condition As Welded As Welded
Tensile Strength 550 MPa (79 ksi) 599 MPa (87 ksi)
Yield Strength 450 MPa (65 ksi) 500 MPa (72 ksi)
Elongation 36 % 32 %

Deposition Data

Current Deposition Rate Diameter Deposition Efficiency (%) Optimal Amps
70-100 A 0.8 kg/h (1.7 lb/h) 2.4 mm (3/32 in.) 66.3 % 90 A
90-160 A 1.2 kg/h (2.6 lb/h) 3.2 mm (1/8 in.) 71.6 % 120 A
130-220 A 1.4 kg/h (3.1 lb/h) 4.0 mm (5/32 in.) 75 % 140 A
130-220 A 1.7 kg/h (3.8 lb/h) 4.0 mm (5/32 in.) 73.5 % 170 A
200-300 A 2.2 kg/h (4.9 lb/h) 4.8 mm (3/16 in.) 76.4 % 200 A
200-300 A 2.4 kg/h (5.4 lb/h) 4.8 mm (3/16 in.) 74.6 % 250 A
90-160 A 1.2 kg/h (2.6 lb/h) 3.2 mm (1/8 in.) 70.9 % 140 A

Classifications

Classifications ASME SFA 5.1 :
AWS A5.1 : E7018-1 H4R
AWS A5.1 : E7018 H4R

Approvals

Approvals ABS 4Y (H5)/AWS A5.1: E7018-1 H4R
CWB CSA W48 E4918-1-H4
DNV/GL 4Y (H5)
LR 4Ym (H5)
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Coating Type Low-hydrogen iron powder
0
Welding Current AC or DC+

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn P S Si
0.05 % 1.20 % 0.01 % 0.008 % 0.45 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Atom Arc 7018 Acclaim
255012056 FIND A DISTRIBUTOR
255012015 FIND A DISTRIBUTOR
255012072 FIND A DISTRIBUTOR
255012031 FIND A DISTRIBUTOR
255012049 FIND A DISTRIBUTOR
255012007 FIND A DISTRIBUTOR
255012064 FIND A DISTRIBUTOR
255012023 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..