Atom Arc 7018-1

ESAB

Atom Arc 7018-1

The following items have been added to your list


x

Atom Arc 7018-1 is an all-position, low hydrogen electrode that provides exceptional impact toughness at low service temperatures. Atom Arc 7018-1 provides smooth metal transfer, minimal spatter, and easy slag removal. Atom Arc 7018-1 is used to join a wide variety of carbon and low alloy steels. It is also an excellent choice for welding higher strength steels if undermatching welds are specified.

BUY NOW


Industries

  • Automotive
  • Civil Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Railcars

Welding Process

  • SMAW/MMA (Stick)

Typical Charpy V-Notch Properties

Stress Relieved
Impact Value 165 ft-lb
Impact Value 224 J
1150 °F
621 °C
8 hr
Testing Temperature -50 °F
Testing Temperature -46 °C

Typical Tensile Properties

Condition Stress Relieved As Welded
Reduction in Area 72 % 72 %
Tensile Strength 510 MPa (74 ksi) 565 MPa (81 ksi)
Yield Strength 415 MPa (60 ksi) 475 MPa (69 ksi)
Elongation 33 % 30 %
Testing Time 8 hr
Testing Temperature 621 degC (1150 degF)

Deposition Data

Current Deposition Rate Diameter Deposition Efficiency (%) Optimal Amps
130-220 A 1.7 kg/h (3.8 lb/h) 4.0 mm (5/32 in.) 73.5 % 170 A
90-160 A 1.2 kg/h (2.6 lb/h) 3.2 mm (1/8 in.) 71.6 % 120 A
200-300 A 2.4 kg/h (5.4 lb/h) 4.8 mm (3/16 in.) 74.6 % 250 A
200-300 A 2.2 kg/h (4.9 lb/h) 4.8 mm (3/16 in.) 76.4 % 200 A
70-100 A 0.8 kg/h (1.7 lb/h) 2.4 mm (3/32 in.) 66.3 % 90 A
90-160 A 1.2 kg/h (2.7 lb/h) 3.2 mm (1/8 in.) 70.9 % 140 A
250-350 A 3.3 kg/h (7.2 lb/h) 5.6 mm (7/32 in.) 74 % 300 A
250-350 A 2.9 kg/h (6.5 lb/h) 5.6 mm (7/32 in.) 75 % 250 A
300-400 A 3.5 kg/h (7.7 lb/h) 6.4 mm (1/4 in.) 78 % 300 A
300-400 A 3.9 kg/h (8.7 lb/h) 6.4 mm (1/4 in.) 77 % 350 A
130-220 A 1.4 kg/h (3.1 lb/h) 4.0 mm (5/32 in.) 75 % 140 A

Classifications

Classifications ASME SFA 5.1 :
AWS A5.1 : E7018-1 H4R

Approvals

Approvals ABS 3,3Y(H10)/A5.1: E7018-1
CWB CSA W48 E4918-1-H4
DNV 3Y(H10)
LR 3m,3Ym(H10)
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Coating Type Low-hydrogen iron powder
0
Welding Current AC or DC+

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn P S Si
0.04 % 1.30 % 0.014 % 0.015 % 0.30 %
0.30 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Atom Arc 7018-1
255011850 FIND A DISTRIBUTOR
255011843 FIND A DISTRIBUTOR
255013146 FIND A DISTRIBUTOR
255013351 FIND A DISTRIBUTOR
255013344 FIND A DISTRIBUTOR
255015356 FIND A DISTRIBUTOR
255015349 FIND A DISTRIBUTOR
255017345 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..