Pipeweld 9010 Plus
Cellulosic coated electrode designed for low alloy steel. Deep penetration welding in all positions, especially in the vertical downward; recommended for welding pipe-lines of API 5LX: X70- X80.
Typical Charpy V-Notch Properties
Impact Value | Testing Temperature | |||
as welded aws | ||||
60 J | -20 degC | |||
35 J | -30 degC | |||
as welded iso | ||||
-20 degC |
Typical Tensile Properties
Condition | As Welded | As Welded |
Shielding Gas | AWS | ISO |
Tensile Strength | 700 MPa | |
Yield Strength | 620 MPa | |
Elongation | 22 % | |
Deposition Data
Current | Deposition Rate | Diameter | Number of electrodes/kg weld metal | Voltage | kg weld metal/kg electrodes | |
65-120 A | 79 sec | 0.82 kg/h | 3.2 x 350 mm | 56 | 32 V | 0.63 |
90-180 A | 78 sec | 1.17 kg/h | 4.0 x 350 mm | 39 | 34 V | 0.63 |
150-240 A | 90 sec | 1.67 kg/h | 5.0 x 350 mm | 24 | 32 V | 0.63 |
Classifications
Classifications |
EN ISO 2560-A : E 50 2 1NiMo C 21 SFA/AWS A5.5 : E9010-P1 |
Approvals
Grade | E 9010-P1 |
Society | FBTS |
Approvals are based on factory location. Please contact ESAB for more information. |
Consumable Characteristics
Alloy Type | Low alloyed (0.9 % Ni, 0.4 % Mo) |
Coating Type | Cellulosic covering |
Welding Current | DC+ |
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Mn | Mo | Ni | Si | ||||||||||
0.10 % | 1.00 % | 0.40 % | 0.90 % | 0.20 % |