Pipeweld 8010 Plus
Cellulosic coated electrode designed for low alloy steel. Deep penetration welding in all positions, especially designed for vertical down welding of high strength pipelines. Provides high economic benefits compared to welding vertical up. Recommended for welding pipe-lines of API 5LX: X60- X70
Typical Charpy V-Notch Properties
Impact Value | Testing Temperature | |||
as welded aws | ||||
40 J | -30 degC | |||
as welded iso | ||||
-20 degC |
Typical Tensile Properties
Condition | As Welded | As Welded |
Shielding Gas | ISO | AWS |
Tensile Strength | 620 MPa | |
Yield Strength | 530 MPa | |
Elongation | 23 % | |
Deposition Data
Current | Deposition Rate | Diameter | Number of electrodes/kg weld metal | Voltage | kg weld metal/kg electrodes | |
65-120 A | 86 sec | 0.68 kg/h | 3.2 x 350 mm | 61 | 30 V | 0.62 |
90-180 A | 84 sec | 1.15 kg/h | 4.0 x 350 mm | 37 | 29 V | 0.68 |
150-240 A | 97 sec | 1.55 kg/h | 5.0 x 350 mm | 24 | 29 V | 0.68 |
Classifications
Classifications |
SFA/AWS A5.5 : E8010-P1 EN ISO 2560-A : E 46 2 Z C 21 |
Approvals
Grade | E 8010-P1 |
Society | FBTS |
Approvals are based on factory location. Please contact ESAB for more information. |
Consumable Characteristics
Alloy Type | Low alloyed (0.3 % Ni, 0.25 % Mo) |
Coating Type | Cellulosic covering |
Welding Current | DC+ |