Pipeweld 7010 Plus
Typical Charpy V-Notch Properties
as welded aws | ||||
Typical Tensile Properties
Condition | Elongation | Shielding Gas | Tensile Strength | Yield Strength |
As Welded | 22 % | AWS | 570 MPa (83 ksi) | 480 MPa (70 ksi) |
Deposition Data
Current | Deposition Rate @ 90% I max | Diameter | Deposition Efficiency (%) | Number of electrodes/kg weld metal | Voltage | |
65-120 A | 90 sec | 0.62 kg/h (1.4 lb/h) | 3.2 x 350.0 mm (1/8 x 13.8 in.) | 58 % | 65 | 31 V |
90-180 A | 93 sec | 0.93 kg/h (2.1 lb/h) | 4.0 x 350.0 mm (5/32 x 13.8 in.) | 59 % | 42 | 30.5 V |
150-240 A | 100 sec | 1.47 kg/h (3.2 lb/h) | 5.0 x 350.0 mm (0.197 x 13.8 in.) | 67 % | 24 | 28.6 V |
Classifications
Classifications |
SFA/AWS A5.5 : E7010-P1 EN ISO 2560-A : E 42 2 Z C 21 |
Approvals
Grade | E 7010-P1 |
Society | FBTS |
Approvals are based on factory location. Please contact ESAB for more information. |
Consumable Characteristics
Alloy Type | Low alloyed (0.3 % Ni, 0.2 % Mo) |
Coating Type | Cellulosic covering |
Welding Current | DC+ |
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Mn | Mo | Ni | Si | ||||||||||
0.09 % | 0.46 % | 0.24 % | 0.34 % | 0.12 % |