Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 22 % 82.7 ksi 69.6 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 40.5 ft-lb -20 °C
As Welded 33 ft-lb -22 °F

Typical Weld Metal Analysis

weld metal analysis
MnMoCSiNi
0.46 %0.24 %0.09 %0.12 %0.34 %

Approvals: FBTS; E 7010-P1
Classifications: SFA/AWS A5.5; E7010-P1; EN ISO 2560-A; E 42 2 Z C 21

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Low alloyed (0.3 % Ni, 0.2 % Mo)
Coating Type: IMPERIAL_Cellulosic covering
Welding Current: DC+
x

Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 22 % 82.7 ksi 69.6 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 40.5 ft-lb -20 °C
As Welded 33 ft-lb -22 °F

Typical Weld Metal Analysis

weld metal analysis
MnMoCSiNi
0.46 %0.24 %0.09 %0.12 %0.34 %

Approvals: FBTS; E 7010-P1
Classifications: SFA/AWS A5.5; E7010-P1; EN ISO 2560-A; E 42 2 Z C 21

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Low alloyed (0.3 % Ni, 0.2 % Mo)
Coating Type: IMPERIAL_Cellulosic covering
Welding Current: DC+
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK PIPEWELD 7010 PLUS
PIPEWELD 7010 PLUS 3.2x350mm 2P70323B40 FIND A DISTRIBUTOR
PIPEWELD 7010 PLUS 4.0x350mm 2P70403B40 FIND A DISTRIBUTOR
PIPEWELD 7010 PLUS 5.0x350mm 2P70503B40 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..