OK B3 SC is a basic AC/DC electrode designed for welding of creep resistant 2,25% Cr 1% Mo alloyed steels, SA-387 Grade 22, A335 Grade P22 or similar materials when highest toughness values are required also after step cooling treatment. Very low level of impurity elements providing a X-bar max. 10 for temper embrittlement resistant applications. Usually welding is followed by a PWHT. Suitable for refinery, petrochemical and chemical industries, power generation, pressure vessels, etc.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
pwht aws
120 J (89 ft-lb) 1 hr 690 degC (1274 degF) -30 degC (-22 degF)
150 J (111 ft-lb) 4 hr 690 degC (1274 degF) -30 degC (-22 degF)
140 J (104 ft-lb) 32 hr 690 degC (1274 degF) -30 degC (-22 degF)

Typical Tensile Properties

Condition PWHT PWHT PWHT PWHT
Test Temp. 454°C
Shielding Gas AWS AWS AWS AWS
Tensile Strength 650 MPa (94 ksi) 650 MPa (94 ksi) 580 MPa (84 ksi) 455 MPa (66 ksi)
Yield Strength 550 MPa (80 ksi) 540 MPa (78 ksi) 460 MPa (67 ksi) 370 MPa (54 ksi)
Elongation 23 % 25 % 27 % 18 %
Testing Time 1 hr 4 hr 32 hr 32 hr
Testing Temperature 690 degC (1274 degF) 690 degC (1274 degF) 690 degC (1274 degF) 690 degC (1274 degF)

Deposition Data

Current Deposition Rate @ 90% I max Diameter Deposition Efficiency (%) Number of electrodes/kg weld metal Voltage
60-95 A 63 sec 0.8 kg/h (1,8 lb/h) 2.5 x 350.0 mm (0.098 x 13,8 in.) 60 % 75 23 V
75-145 A 62 sec 1.2 kg/h (2,6 lb/h) 3.2 x 350.0 mm (1/8 x 13,8 in.) 60 % 48 23 V
100-200 A 86 sec 1.7 kg/h (3,7 lb/h) 4.0 x 450.0 mm (5/32 x 17,7 in.) 58 % 25 26 V
115-260 A 106 sec 2.3 kg/h (5,1 lb/h) 5.0 x 450.0 mm (0.197 x 17,7 in.) 63 % 15 25 V

Classifications

Weld Metal SFA/AWS A5.5 : E9018-B3 H4 R
EN ISO 3580-A : E CrMo2 B 32 H5

Approvals

Approvals CE EN 13479
VdTÜV 19612
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Low alloyed (2.25% Cr ; 1% Mo)
Coating Type Basic covering
Diffusible Hydrogen < 4.0 ml/100g
Welding Current DC+-, AC

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
Al As B C Cr Cu J-Factor Mn Mn+Si Mo Nb Nb+Ti+V Ni P P+Sn PE S Sb Si Sn Ti V X-bar
0.002 % 0.002 % 0.0002 % 0.085 % 2.35 % 0.04 % 70 % 0.7 % 0.9 % 1 % 0.004 % 0.018 % 0.04 % 0.005 % 0.009 % 2.7 % 0.004 % 0.001 % 0.20 % 0.004 % 0.007 % 0.007 % 7 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK B3 SC
76242530G0 FIND A DISTRIBUTOR
76243230G0 FIND A DISTRIBUTOR
76244040G0 FIND A DISTRIBUTOR
76245040G0 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..