This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next
ESAB

WEAR-ARC 6 IP

WEAR-ARC 6 IP

The iron powder low hydrogen coating of Wear-Arc 6-IP electrodes promotes good bonds with manganese and carbon steels. Wear-Arc 6-IP is recommended for the reclamation of parts subject to wear caused by abrasion and light impact. This electrode is ideal for field work where parts cannot be positioned for downhand welding. Typical applications are: Shovel buckets and teeth, Dragline buckets and teeth, Pug mill paddles, Tamping tools, Screens, Asphalt mixer paddles, Crushing equipment, Granulators, Trunnions, Truck bodies.

Where To Buy


Industries

  • Mobile Equipment
  • Railcars
  • Steel Industry
  • Industrial and General Fabrication

Welding Process

  • SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Hardness (HRC)
As Welded 58 HRC

Typical Weld Metal Analysis %

weld metal analysis
MnCSiCr
0.80 %3.00 %1.80 %6.50 %

Classifications: No AWS Classification

x

Typical Tensile Properties

Condition Hardness (HRC)
As Welded 58 HRC

Typical Weld Metal Analysis %

weld metal analysis
MnCSiCr
0.80 %3.00 %1.80 %6.50 %

Classifications: No AWS Classification

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : WEAR-ARC 6 IP
WA 6-IP 5/32X14X10#HS 259035301 Buy Local
WA 6-IP 3/16X14X10#HS 259033108 Buy Local
WA 6-IP 1/8X14X10#HS 259031805 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..