WEAR-ARC 4 IP

WEAR-ARC 4 IP

Wear-Arc 4-IP is an all position, iron powder, low hydrogen hardsurfacing electrode providing sound overlays on carbon and low alloy steels, as well as many abrasion-resistant steels. The low hydrogen coating of this electrode promotes excellent fusion with the above steels and on buildup alloys without underbead cracking. This product is designed to provide hard, deformation-resistant, crack-free weld metal for resistance to metal-to-metal wear involving impact, compression, and abrasion. Typical applications are: dragline bucket pins and links, dredge bucket lips, dredge driving tumblers, dredge spud points, can brake drums, mill brake drums, shovel idlers, cable sheaves, cable sheave shafts, elevator bucket lips, shovel rollers, shovel latch pins and keepers, tractor idlers, tractor rollers, wheels (mine car, skip car, etc.), ditcher drive segments, ditcher rollers, shovel boom heels.

Where To Buy


Industries

  • Mobile Equipment
  • Railcars
  • Steel Industry
  • Industrial and General Fabrication

Welding Process

  • SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Hardness (HRC)
As Welded 55 HRC

Typical Weld Metal Analysis %

MnMoCSiCr
0.90 %1.00 %0.40 %1.30 %2.20 %

Classifications: No AWS Classification

x

Typical Tensile Properties

Condition Hardness (HRC)
As Welded 55 HRC

Typical Weld Metal Analysis %

MnMoCSiCr
0.90 %1.00 %0.40 %1.30 %2.20 %

Classifications: No AWS Classification

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : WEAR-ARC 4 IP
WA 4-IP 1/8X14X10#HS 259021806 Buy Local
WA 4-IP 3/16X14X10#HS 259023109 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..