Stoody

Stoody X-53

Stoody X-53

Stoody X-53 is a hardfacing electrode that combines the desired features of high deposition rate, high bead build up, and resistance to impact and abrasion. It can be used to overlay carbon or manganese steel parts.

Where To Buy


Features

  • Deposits are not machinable or forgeable.

Specifications


Typical Tensile Properties

Hardness (HRC)
50-54 HRC

Typical Weld Metal Analysis %

OtherCCrFe
4.0 %3.5 %15.5 %BAL %

x

Typical Tensile Properties

Hardness (HRC)
50-54 HRC

Typical Weld Metal Analysis %

OtherCCrFe
4.0 %3.5 %15.5 %BAL %