Stoody Versalloy Plus
Stoody Versalloy Plus coated electrode is a modified austenitic stainless steel recommended for joining, rebuilding, or cushion-overlaying on applications involving high strength, heat, and corrosion resistance.
Features
- It is frequently used in dissimilar metal applications to join carbon steels to stainless steels.
- Versalloy Plus has excellent welder appeal with a smooth semi-spray arc and self-peeling slag.
Typical Tensile Properties
Elongation | Tensile Strength | Yield Strength |
22 % | 800 MPa (116 ksi) | 621 MPa (90 ksi) |
Deposition Data
Current | Deposition Type | Diameter |
50-90 A | Full Range | 2.4 mm (3/32 in.) |
75-125 A | Full Range | 3.2 mm (1/8 in.) |
90-150 A | Full Range | 4.0 mm (5/32 in.) |
Typical Weld Metal Analysis %
C | Cr | Fe | Other |
0.1 % | 28.0 % | BAL % | 12.0 % |