Stoody Super 20 is a solid core electrode with a heavy extruded coating that contains the alloying elements. The product's extremely good wear resistance is attributed to the addition of molybdenum, tungsten, and chromium. It can be used in hot wear service up to 1100° F (593° C). The abrasion resistance of this alloy approaches that of a tungsten carbide and thus has been given the name "the poor man's tungsten carbide".

BUY NOW


Features

  • IDeposits will cross check and should be limited to one layer.
  • The deposits are not machinable or forgeable.


Typical Tensile Properties

58-63 HRC 60-65 HRC

Deposition Data

Current Deposition Type Diameter
70-160 A - Full Range 3.2 mm (1/8 in.) - - -
130-250 A - Full Range 4.0 mm (5/32 in.) - - -
200-300 A - Full Range 4.8 mm (3/16 in.) - - -

Typical Weld Metal Analysis %

C Cr Fe Other
6.0 % 21.0 % BAL % 8.0 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Stoody Super 20
1/8 in / 3.2 mm x 14 Super 20 CTD 10lb Pak 46520810 FIND A DISTRIBUTOR
3/16 in / 4.8 mm x 14 Super 20 CTD 10lb Pak 46521210 FIND A DISTRIBUTOR
5/32 in / 4.0 mm x 14 Super 20 CTD 10lb Pak 46521010 FIND A DISTRIBUTOR
x
x

x

Loading..