Stoody Self-Hardening is a general purpose solid core hardfacing electrode that offers a good balance of impact and abrasion resistance. It can be used on both metal-to-metal and metal-to-earth applications.

BUY NOW


Features

  • Self-Hardening can be applied to carbon and low alloy steels. It can be forged at red heat, but it is not readily machinable.

Typical Tensile Properties

Deposition Data

Current Deposition Type Diameter
100-150 A Full Range 3.2 mm (1/8 in.)
150-200 A Full Range 4.0 mm (5/32 in.)
175-275 A Full Range 4.8 mm (3/16 in.)

Typical Weld Metal Analysis %

C Cr Fe Other
1.0 % 8.5 % BAL % 2.0 %