Stoody

Stoody Foundry Co-Mang

Stoody Foundry Co-Mang

Foundry Co-Mang is a manganese steel coated electrode. It is suitable for multi-layer build-up and has excellent work hardening characteristics.

Where To Buy


Features

  • It is usable for austenitic manganese steel repair, buildup, and joining.

Specifications


Typical Tensile Properties

Elongation Hardness (BHN) Tensile Strength Yield Strength
42 % 350-450 BHN 128 ksi 71 ksi

Typical Weld Metal Analysis %

OtherMnCFe
1.0 %16.0 %1.0 %BAL %

x

Typical Tensile Properties

Elongation Hardness (BHN) Tensile Strength Yield Strength
42 % 350-450 BHN 128 ksi 71 ksi

Typical Weld Metal Analysis %

OtherMnCFe
1.0 %16.0 %1.0 %BAL %

x
x
×