Stoody 60

Stoody 60 is a nickel based alloy with the same properties as Stoody 50, but produces a harder and more wear resistant deposit. Certification to AWS specification - A5.21 ERNiCr-C

Where To Buy


Features

Certification to AWS specification - A5.21 ERNiCr-C. Stoodite cobalt base and nickel base alloys are manufactured to conform to the chemistry and usability requirements of the specifications noted. Certification to ASME and MIL must be requested at the time order is placed and must appear on the written P.O. Additional charges apply for military, nuclear, or special certification requirements.

  • Hard, wear resistant deposit
  • Grind finish, not machinable


Specifications


Typical Tensile Properties

Hardness (HRC)
56-58 HRC

Typical Weld Metal Analysis %

OtherCNiCrFe
7.5 %1.0 %BAL %12.5 %4.5 %

Classifications: AWS A5.21; ERNiCr-C

x

Typical Tensile Properties

Hardness (HRC)
56-58 HRC

Typical Weld Metal Analysis %

OtherCNiCrFe
7.5 %1.0 %BAL %12.5 %4.5 %

Classifications: AWS A5.21; ERNiCr-C