Stoody 2134
Stoody 2134 exhibits excellent abrasion resistance in fine, sandy soils, and bonds well with carbon, low alloy, and manganese steels. It is tubular electrode containing granular alloying elements. The coating is graphitic.
Features
- Deposits are not machinable or forgeable.
- Stoody® 2134 can be used in hot wear applications up to 950F.
Typical Tensile Properties
Deposition Data
Current | Deposition Type | Diameter |
150-210 A | Full Range | 4.8 mm (3/16 in.) |
110-170 A | Full Range | 4.0 mm (5/32 in.) |
180-300 A | Full Range | 6.4 mm (1/4 in.) |
Typical Weld Metal Analysis %
C | Cr | Fe | Other |
4.0 % | 25.0 % | BAL % | 7.0 % |