Stoody 1105

Stoody

Stoody 1105

The following items have been added to your list


x

Stoody 1105 LH is a solid core electrode designed for wear resistance in metal-to-metal applications. It has an extruded coating containing the alloying elements. It provides good weldability and a high deposition rate. It bonds readily to carbon and low alloy steels and is not recommended for manganese steels or cast irons. It is forgeable at red heat.

BUY NOW


Typical Tensile Properties

Deposition Data

Current Deposition Type Diameter
80-150 A - Full Range 3.2 mm (1/8 in.) - - -
140-210 A - Full Range 4.0 mm (5/32 in.) - - -
165-250 A - Full Range 4.8 mm (3/16 in.) - - -

Typical Weld Metal Analysis %

C Cr Fe Other
0.5 % 3.0 % BAL % 2.0 %