Stoody 1102

Stoody

Stoody 1102

The following items have been added to your list


x

Stoody 1102 is an electrode with a solid core wire designed for wear resistance in metal-to-metal applications. It has an extruded coating containing the alloying elements. Stoody 1102 has an all-weld-metal composition and physical properties that are similar to those of H-12 tool steel. Weldability is very good and it can be applied in all positions. Stoody 1102 requires carbide tools for machining. It is good for hot wear applications up to 1100° F (595° C). Multiple layers can be applied without difficulty when proper preheat and interpass temperatures, and cooling rates are controlled.

BUY NOW


Typical Tensile Properties

Deposition Data

Current 125-150 A
Deposition Type 3
Diameter 1/8 in.
Diameter 3.2 mm

Typical Weld Metal Analysis %

C Cr Fe Other
0.5 % 5.5 % BAL % 3.0 %