Stoody

Stoodite 6H

Stoodite 6H

Stoodite 6H, like its base product Stoodite 6, provides resistance to many forms of chemical and mechanical degradation over a wide temperature range. While the chemistry of Stoodite 6H will fall within that prescribed for the base product, several elements have been more closely controlled to provide better transfer across an arc, thus yielding a smoother gas tungsten arc deposit. The premium alloy has outstanding consistency, anti-galling properties, high temperature hardness, and high resistance to cavitation erosion. Stoodite 6H bonds well with weldable grade steels including stainless. Can be certified to AWS specification - A5.21 ERCoCr-A

Where To Buy


Features

Can be certified to AWS specification - A5.21 ERCoCr-A. Stoodite cobalt base alloys are manufactured to conform to the chemistry and usability requirements of the specifications noted. Certification to ASME and MIL must be requested at the time order is placed and must appear on the written P.O. Additional charges apply for military, nuclear, or special certification requirements.

  • Good balance of abrasion and impact resistance
  • Excellent resistance to many forms of mechanical and chemical degradation over a wide temperature range
  • Outstanding self-mated anti-galling properties
  • High temperature hardness
  • Resistance to cavitation erosion
  • Machinable with carbide tools
  • Bonds well with weldable alloy steels, including stainless


Specifications


Typical Tensile Properties

Hardness (HRC)
40-48 HRC

Typical Weld Metal Analysis %

MnMoCSiWNiCoCrFe
0.09 %0.1 %1.3 %1.3 %5.5 %1.0 %BAL %30.6 %1.0 %

Classifications: AWS A5.21; ERCoCr-A; MIL R-17131C Amd 1, Type MIL-RCoCr-A-3

x

Typical Tensile Properties

Hardness (HRC)
40-48 HRC

Typical Weld Metal Analysis %

MnMoCSiWNiCoCrFe
0.09 %0.1 %1.3 %1.3 %5.5 %1.0 %BAL %30.6 %1.0 %

Classifications: AWS A5.21; ERCoCr-A; MIL R-17131C Amd 1, Type MIL-RCoCr-A-3