Stoody

Stoodite 12

Stoodite 12

Stoodite 12 is similar to Stoodite 6 in composition with the most significant difference being carbide volume. Stoodite 12 has high hardness and abrasion resistance. Non-magnetic and non-forgeable, the alloy can be machined with great difficulty using carbide tools. Stoodite 12 bonds well with weldable alloy steels, including stainless. Can be certified to AWS specification - A5.21 ERCoCr-B for bare rods; A5.13 ECoCr-B for coated electrodes.

Where To Buy


Features

Can be certified to AWS specification - A5.21 ERCoCr-B for bare rods; A5.13 ECoCr-B for coated electrodes. Stoodite cobalt base alloys are manufactured to conform to the chemistry and usability requirements of the specifications noted. Certification to ASME and MIL must be requested at the time order is placed and must appear on the written P.O. Additional charges apply for military, nuclear, or special certification requirements.

  • High hardness and abrasion resistance
  • Bonds well with weldable alloy steels, including stainless


Specifications


Typical Tensile Properties

Hardness (HRC)
46-48 HRC

Typical Weld Metal Analysis %

MnMoCSiWNiCoCrFe
0.1 %0.1 %1.3 %0.9 %8.0 %2.0 %BAL %29.8 %3.3 %

Classifications: AWS A5.21; ERCoCr-B; AWS A5.13; ECoCr-B

x

Typical Tensile Properties

Hardness (HRC)
46-48 HRC

Typical Weld Metal Analysis %

MnMoCSiWNiCoCrFe
0.1 %0.1 %1.3 %0.9 %8.0 %2.0 %BAL %29.8 %3.3 %

Classifications: AWS A5.21; ERCoCr-B; AWS A5.13; ECoCr-B

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Stoodite 12
1/8 in / 3.2 mm x 14 Stoodite 12 Bare 5lb Tube 11406700 Buy Local
5/32 in / 4.0 mm x 14 Stoodite 12 CTD 10lb Vacpak 811211205156 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..