Stoody

Stoody Castweld 55

The following items have been added to your list


x

Stoody Castweld 55 is used on worn cast iron parts requiring build up or joining but not needing tight dimensional control or machining.

BUY NOW


Features

  • Castweld 55 has good tolerance for the high phosphorus often found in cast iron to dissimilar metals.

Deposition Data

Current Deposition Type Diameter
40-80 A Full Range 2.4 mm (3/32 in.)
70-110 A Full Range 3.2 mm (1/8 in.)
100-140 A Full Range 4.0 mm (5/32 in.)

Classifications

Grade ENiFe-CI-A
Name AWS A5.15-90

Typical Weld Metal Analysis %

C Fe Mn Ni Si
1.3 % BAL % 0.6 % 49.0 % 0.8 %