ESAB’s new iSeries technology provides the next generation of higher productivity, increased flexibility and confidence in high precision plasma cutting. Superior performance on mild steel and non-ferrous metals will meet or exceed other systems in its class. Designed to grow with your business, you can upgrade your system in minutes. The iSeries systems utilize StepUp™ modular power technology, allowing units to be easily upgraded -ensuring you always have the right amount of power for your current and future applications. Now up to 800 A for stainless steel and aluminum.

BUY NOW


Features

  • HeavyCut™ provides the best cut quality, precision and parts life with XTremeLife™ Wear Parts
  • Unmatched cut quality on non-ferrous metals using unique Water Mist Secondary (WMS®) process up to 800 A
  • Highest cut speed in its class on stainless steel –up to 3 times faster than similar cutting systems
  • Work pieces can go directly from the cutting table to welding, painting or assembly without expensive secondary operations
  • Excellent dross-free cuts using oxygen (O2) plasma on mild steel
  • Production cutting on stainless steel and aluminum up to 160 mm (6-3/8 in.), now up to 800 A


Industries

  • Railcars
  • Heavy Fabrication
  • Marine and Offshore
  • General Manufacturing

Dimensions

Dimensions 1219 x 698 x 1031 mm (48.0 x 27.5 x 40.6 in.)

Cutting Specifications

Model 100i 200i 300i 400i 600i 800i
Mild Steel
Recommended Cut 12 mm (1/2 in.) 25 mm (1 in.) 40 mm (1 1/2 in.) 50 mm (2 in.) 50 mm (2 in.) 50 mm (2 in.)
Maximum Cut 15 mm (5/8 in.) 40 mm (1 1/2 in.) 45 mm (1 3/4 in.) 50 mm (2 in.) 50 mm (2 in.) 50 mm (2 in.)
Maximum Edge Start 20 mm (3/4 in.) 65 mm (2 1/2 in.) 75 mm (3 in.) 90 mm (3 1/2 in.) 90 mm (3 1/2 in.) 90 mm (3 1/2 in.)
Stainless Steel
Recommended Cut 12 mm (1/2 in.) 25 mm (1 in.) 30 mm (1 1/4 in.) 50 mm (2 in.) 75 mm (3 in.) 90 mm (3 1/2 in.)
Maximum Cut 15 mm (5/8 in.) 25 mm (1 1/2 in.) 30 mm (1 1/4 in.) 50 mm (2 in.) 75 mm (3 in.) 90 mm (3 1/2 in.)
Maximum Edge Start 20 mm (3/4 in.) 50 mm (2 1/2 in.) 50 mm (2 in.) 100 mm (4 in.) 100 mm (4 in.) 160 mm (6 1/4 in.)
Aluminium
Recommended Cut 12 mm (1/2 in.) 20 mm (3/4 in.) 25 mm (1 in.) 50 mm (2 in.) 75 mm (3 in.) 90 mm (3 1/2 in.)
Maximum Cut 15 mm (5/8 in.) 25 mm (1 in.) 30 mm (1 1/4 in.) 60 mm (2 1/2 in.) 75 mm (3 in.) 90 mm (3 1/2 in.)
Maximum Edge Start 20 mm (3/4 in.) 50 mm (2 in.) 50 mm (2 in.) 90 mm (3 1/2 in.) 100 mm (4 in.) 160 mm (6 1/4 in.)

Operating Specifications

Enclosure Class CSA, CE, CCC

Weight

100i 200i 300i 400i 600i 800i 100i 200i 300i 400i 600i 800i 100i 200i 300i 400i 600i 800i
Description or Qualifier 380-480 V 380-480 V 380-480 V 380-480 V 380-480 V 380-480 V 230 V 230 V 230 V 230 V 230 V 230 V 600 V 600 V 600 V 600 V 600 V 600 V
Weight 186 kg (410 lb) 205 kg (451 lb) 224 (x2) kg (537 (x2) lb) 252 kg (555 lb) 224 (x2) kg (537 (x2) lb) 252 (x2) kg (555 (x2) lb) 336 kg (740 lb) 455 kg (1001 lb) 555 kg (1220 lb) 555 (x2) kg (1220 (x2) lb) 296 kg (652 lb) 326 kg (718 lb) 356 kg (783 lb) 386 kg (849 lb) 356 (x2) kg (783 (x2) lb) 386 (x2) kg (849 (x2) lb)

Input Ratings

Model 100i 200i 300i 400i 600i 800i
Amps 61 A @ 230 V
43 A @ 380 V
41 A @ 400 V
34 A @ 480 V
23 A @ 600 V
65 A @ 380 V
62 A @ 400 V
52 A @ 480 V
121 A @ 230 V
45 A @ 600 V
97 A @ 380 V
93 A @ 400 V
77 A @ 480 V
194 A @ 230 V
73 A @ 600 V
144 A @ 380 V
137 A @ 400 V
114 A @ 480 V
96 A @ 600 V
388 A @ 230 V
194 A @ 380 V
186 A @ 400 V
154 A @ 480 V
146 A @ 600 V
288 A @ 380 V
274 A @ 400 V
228 A @ 480 V
192 A @ 600 V
Frequency Hz 50/60 Hz 50/60 Hz 50/60 Hz 50/60 Hz 50/60 Hz 50/60 Hz
Phase 3 3 3 3 3 3

Output Ratings

Model 100i 200i 300i 400i 600i 800i
Amp High 100 A
200 A
300 A
400 A
600 A
800 A
Amp Low 5 A
5 A
5 A
5 A
5 A
5 A
Duty Cycle 100 %
100 %
100 %
100 %
100 %
100 %
Output Power 20 kW
40 kW
60 kW
80 kW
120 kW
160 kW

Extra Info