Arcair Professional Angle-Arc® K3000 is part of the manual gouging torch & cable assemblies offered by the industry leader in the air carbon-arc products.

BUY NOW


Features

  • IMPROVED TORCH AIR FLOW - More efficient use of air supply. Improved metal removal.
  • FOUR HOLE HEAD ASSEMBLY - Optimizes air flow to the arc. Efficiently cleans slag from groove edge.
  • AIR ASSIST POSITIVE AIR SHUT-OFF - Minimizes air supply unit cycling on and off. Allows torch usage when air supply is marginal.
  • IMPROVED CABLE ELECTRICAL CONDUCTION - Improves cable service life. Decreases heat build up in cable and torch.
  • SUPERIOR OUTER CABLE COVER - Durable cover for improved cable life in a harsh environment. Resists breakdown due to exposure to heat produced by gouging.
  • INSULATED CONNECTION BOOT & HOOK-UP KIT - Makes for easy torch hook-up. Virtually eliminates the possibility of arcing when contacting electrically hot parts.


Arc Gouging Specs

Model 01065001 01065001 01065001 01065001 01065001 61065002 61065002 61065002 61065002 61065002 61065003 61065003 61065003 61065003 61065003 61065006 61065006 61065006 61065006 61065006 61065007 61065007 61065007 61065007 61065007
Conditional Statement Pointed Jointed Flat Half Round Pointed Jointed Flat Half Round Pointed Jointed Flat Half Round Pointed Jointed Flat Half Round Pointed Jointed Flat Half Round
Carbon Electrode Range 3.2-9.5 mm (1/8-3/8 in.) 7.9-9.5 mm (5/16-3/8 in.) 9.5-15.9 mm (3/8 and 5/8 in.) 15.9 mm (5/8 in.) 3.2-9.5 mm (1/8-3/8 in.) 7.9-9.5 mm (5/16-3/8 in.) 9.5-15.9 mm (3/8 and 5/8 in.) 15.9 mm (5/8 in.) 3.2-9.5 mm (1/8-3/8 in.) 7.9-9.5 mm (5/16-3/8 in.) 9.5-15.9 mm (3/8 and 5/8 in.) 15.9 mm (5/8 in.) 3.2-9.5 mm (1/8-3/8 in.) 7.9-9.5 mm (5/16-3/8 in.) 9.5-15.9 mm (3/8 and 5/8 in.) 15.9 mm (5/8 in.) 3.2-9.5 mm (1/8-3/8 in.) 7.9-9.5 mm (5/16-3/8 in.) 9.5-15.9 mm (3/8 and 5/8 in.) 15.9 mm (5/8 in.)
Air Requirement 5.6 (80 psi) 5.6 (80 psi) 5.6 (80 psi) 5.6 (80 psi) 5.6 (80 psi)
Flow Rate 624 l/min (22 cfh) 624 l/min (22 cfh) 624 l/min (22 cfh) 624 l/min (22 cfh) 624 l/min (22 cfh)

Arc Gouging Consumables

Amperage Capacity Up to 600 A
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Professional Angle-Arc K3000
70088110
70088107
61065007
61065006
61065003
61065002