Stoody® Introduces New All-Position Flux-Cored Nickel Alloy Wire

Stoody 625-T1C is an all-position Flux-Cored nickel alloy wire designed to weld with 100% CO2 shielding. It can be used for joining and cladding of nickel alloys, stainless steels as well as 9% Ni steel used to build liquefied natural gas (LNG) tanks. The composition of Stoody 625-T1C wire results in an all-weld deposit with iron content below 1%, which is essential for applications requiring enhanced corrosion resistance.

Stoody 625-T1C is available in 0.045" (1.2 mm) diameter on 33 lb. (15 kg) wire baskets.  Classifications include AWS A5.34/A5.34M:2013; ENiCrMo3T1-1; and, ISO: TNi 6625-11.

For more information on product specifications and packaging, including detailed product data sheets, visit stoody.com.  