52 Submerged Arc Flux & Wire Agency Approvals* (cont’d.) Unionmelt Wires Fluxes AWS CWB ABS Military Others 120 709-5 F11A6-EM4-G Alloy Shield M2S 651VF F11A6-ECM2-M2 Alloy Shield M3S 651VF F11A4-ECM3-M3 F2S 709-5 F10P2-ECF2-F2 WS 429 F7A2, F8A2-EW-W St. Hwy - F7A2, F8A2-EW-WH8 F8A2-EW-WH8 709-5 F7A2, St. Hwy - F7A2, F8A2-EW-WH8 F8A2-EW-WH8 439 F7A4, St. Hwy - F7A4, F8A4-EW-WH8 F8A4-EW-WH8 656 F7A5-EW-WH8 St. Hwy - F7A5, EW-WH8 Alloy Shield WS 651VF F7A4-ECW-W * Approvals are subject to change without notice. Consult Marketing for the latest approval revisions.