Bare corrosion resisting chromium-nickel rods for welding of austenitic chromium nickel alloys of 18% Cr 8% Ni-type. OK Tigrod 308LSi has a good general corrosion resistance. The alloy has a low carbon content which makes this alloy particularly recommended were there is a risk of intergranular corrosion. The higher silicon content improves the welding properties, such as wetting. The alloy is widely used in the chemical and food processing industries as well as for pipes, tubes and boilers.

BUY NOW


Vrubová houževnatost

po svaření

Typické vlastnosti v tahu

Mez pevnosti v tahu Mez skluzu PodmínkyProdloužení
635 MPa (92 ksi)480 MPa (70 ksi)Po svaření37 %

Klasifikace

Wire Electrode SFA/AWS A5.9 : ER308LSi
Werkstoffnummer : ~1.4316
EN ISO 14343-A : W 19 9 L Si

Schválení

Schválení BV 308L BT
CE EN 13479
DB 43.039.11
DNV-GL VL 308 L (I1)
NAKS/HAKC 1.6MM-3.2MM
VdTÜV 05335
Schválení jsou platná podle místa výroby. Prosím kontaktujte ESAB pro další informace.

Charakteristika svařovacího materiálu

Typ legování Austenitic (with approx. 8 % ferrite) 19% Cr - 9% Ni - Low C
Ochranný plyn I1 (EN ISO 14175)

Chemické složení svarového kovu

Typického chemické složení svarového kovu v %
C Cr Cu FN WRC-92 Mn Mo N Nb Ni P S Si
0.01 % 20 % 0.1 % 8 % 1.8 % 0.1 % 0.07 % 0.1 % 10 % 0.02 % 0.01 % 0.7 %
Typical Wire Composition %
0.01 % 20.0 % 0.10 % 8 % 1.8 % 0.1 % 0.06 % 0.02 % 10.0 % 0.013 % 0.012 % 0.8 %
x

Objednací číslo a příslušenství

Objednací číslo : OK Tigrod 308LSi
161210R150 FIND A DISTRIBUTOR
161212R150 FIND A DISTRIBUTOR
161216R150
161220R150 FIND A DISTRIBUTOR
161224R150
161232R150 FIND A DISTRIBUTOR
161240R150 FIND A DISTRIBUTOR
x
x

x

Loading..