Agglomerated aluminate-basic flux for Submerged Arc Welding. General purpose flux with excellent welding performance, suitable for all kinds of steels. High impact toughness values. Fits to a large range of SAW wires. For general constructions, pressure vessels, shipbuilding, pipe mills, wind tower productions, transport industries, etc. Designed for single and multi wire procedures, for butt and fillet welds. Suitable for DC and AC welding. Single layer and multi layer welding of unlimited plate thickness.

BUY NOW


Klasifikace

Jakost S A AB 1 67 AC H5
Název EN ISO 14174

Schválení

Schválení CE EN 13479
DB 51.039.05
PL,RU : NAKS/HAKC RD 03-613-03
Schválení jsou platná podle místa výroby. Prosím kontaktujte ESAB pro další informace.

Charakteristika svařovacího materiálu

Změna legování Slightly Silicon and moderately Manganese alloying
Index bazicity nom: 1.5
Hustota nom: 1.2 kg/dm3
Difuzní vodík max 5 ml H/100g weld metal (Redried flux)
Velikost zrna 0.2-1.6 mm (10x65 mesh) or 0.315 -2.0 mm (9x48 mesh)
Typ strusky Aluminate-basic

Spotřeba tavidla

V Hmotnost tavidla/1kg, drát DC Hmotnost tavidla/1kg, drát AC
26 V 0.7 kg 0.6 kg
30 V 1.0 kg 0.9 kg
34 V 1.3 kg 1.2 kg
38 V 1.6 kg 1.4 kg
A Rozměry Rychlost přesunu
580 A Ø 4.0 mm 55 cm/min

Klasifikace

Svařovací drát AWS/EN EN - po svaření Po svaření PWHT
OK Autrod 12.20 A5.17:EM12/ 14171-A:S2 14171-A: S 38 4 AB S2 A5.17: F7A4-EM12 A5.17: F6P4-EM12
OK Autrod 12.10 A5.17:EL12/ 14171-A:S1 14171-A: S 35 4 AB S1 A5.17: F6A4-EL12 A5.17: F6P5-EL12
OK Autrod 12.22 A5.17:EM12K/ 14171-A:S2Si 14171-A: S 38 4 AB S2Si A5.17: F7A5-EM12K A5.17: F6P5-EM12K
OK Autrod 12.34 A5.23:EA4/ 14171-A:S3Mo; 24598-A:S S MnMo 14171-A: S 50 3 AB S3Mo A5.23: F8A4-EA4-A3 A5.23: F8P2-EA4-A3
OK Autrod 12.32 A5.17:EH12K/ 14171-A:S3Si 14171-A: S 46 4 AB S3Si A5.17: F7A5-EH12K A5.17: F7P5-EH12K
OK Autrod 13.27 A5.23:ENi2/ 14171-A:S2Ni2 14171-A: S 46 5 AB S2Ni2 A5.23: F8A6-ENi2-Ni2 A5.23: F7P6-ENi2-Ni2
OK Autrod 13.24 A5.23:ENi6/ 14171-A:S3Ni1Mo0,2 14171-A: S 50 4 AB S3Ni1Mo0,2 A5.23: F8A5-ENi6-Ni6 A5.23: F8P4-ENi6-Ni6
OK Autrod 12.24 A5.23:EA2/ 14171-A:S2Mo; 24598-A:S S Mo 14171-A: S 46 2 AB S2Mo A5.23: F8A2-EA2-A4 A5.23: F7P0-EA2-A4
OK Autrod 12.30 14171-A:S3 14171-A: S 46 3 AB S3 -
OK Autrod 13.36 A5.23:EG/ 14171-A:S2Ni1Cu 14171-A: S 46 3 AB S2Ni1Cu A5.23: F8A2-EG-G
OK Autrod 13.64 A5.23:EA2TiB/ 14171-A:S2MoTiB A5.23: F8TA6-EA2TiB
OK Autrod 13.62 A5.23:EG/ 14171-A:SZ3TiB -
OK Autrod 12.22L A5.17:EM12K/ 14171-B:SU21 A5.17: F7A4-EM12K A5.17: F6P5-EM12K
ESAB SA10K A5.17:EH10K A5.17: F7A4-EH10K A5.17: F7P6-EH10K
OK Autrod 12.08L A5.17:EL8/EL12/ 14171-A:S1 A5.17: F6A2-EL8
OK Autrod 12.24L A5.23:EA2/ 14171-B:SU2M3 A5.23: F8A2-EA2-A4 A5.23: F7P0-EA2-A4
OK Autrod 12.33L A5.23:EA3K A5.23: F9A0-EA3K-G A5.23: F8P0-EA3K-G
OK Autrod 12.40L A5.17:EH14/ 14171-B:SU41 A5.17: F7A4-EH14 A5.17: F7P5-EH14

Schválení

Svařovací drát ABS BV CE ClassNK DB DNV GL IBR IRS LR M N Dastur PRS RINA RS VdTÜV
OK Autrod 12.08L * - - - - - - - * - - - - - -
OK Autrod 12.10 * * * - * * * - - * - * - * *
OK Autrod 12.20 * * * - * * * - - * - * * * *
OK Autrod 12.22 * * * * * * * - - * - - - * *
OK Autrod 12.22L - - - - - - - - - * - - - - -
OK Autrod 12.24 * * * * * * * - - * - * * * *
OK Autrod 12.30 - - * - * - - - - - - - - - *
OK Autrod 12.32 - - * - * - - - - - - - - - *
OK Autrod 12.40L - - - - - * - * * * * - - - -
OK Autrod 13.27 - - - - - - - - - - - - - - *
OK Autrod 13.36 - - * - - - - - - - - - - - -
*Pouze pro vybraný výrobní závod. Pro další informace prosím kontaktujte ESAB. Navštivte stránky esab.com a stáhněte si materiálový list konkrétní kombinaci tavidlo/drát kde jsou uvedeny potřebné detaily.

Typické mechanické vlastnosti

Svařovací drát Podmínky Mez skluzu Mez pevnosti v tahu Zkouška rázem Prodloužení Doba testu
ESAB SA10K PWHT DC+ 430 MPa
(62 ksi),410 MPa
(59 ksi)
530 MPa
(77 ksi),500 MPa
(73 ksi)
120 J @ -18°C,
(89 ft-lb @ -0.4 °F)
100 J @ -29°C,
(74 ft-lb @ -20.2 °F)
75 J @ -40°C,
(56 ft-lb @ -40 °F)
40 J @ -51°C,
(30 ft-lb @ -59.8 °F)
40 J @ -29°C,
(30 ft-lb @ -20.2 °F)
32 %,34 % 1 hr,5 hr
ESAB SA10K Po svaření DC+ 490 MPa
(71 ksi)
580 MPa
(84 ksi)
70 J @ -18°C,
(52 ft-lb @ -0.4 °F)
45 J @ -29°C,
(33 ft-lb @ -20.2 °F)
30 J @ -40°C,
(22 ft-lb @ -40 °F)
26 %
OK Autrod 12.08L PWHT DC+ 300 MPa
(44 ksi)
390 MPa
(57 ksi)
125 J @ 0°C,
(93 ft-lb @ 32 °F)
110 J @ -18°C,
(81 ft-lb @ -0.4 °F)
80 J @ -29°C,
(59 ft-lb @ -20.2 °F)
35 % 1 hr
OK Autrod 12.08L Po svaření DC+ 390 MPa
(57 ksi)
450 MPa
(65 ksi)
120 J @ 0°C,
(89 ft-lb @ 32 °F)
100 J @ -18°C,
(74 ft-lb @ -0.4 °F)
70 J @ -29°C,
(52 ft-lb @ -20.2 °F)
25 %
OK Autrod 12.10 Po svaření AWS DC+ 360 MPa
(52 ksi)
465 MPa
(67 ksi)
125 J @ 0°C,
(93 ft-lb @ 0 °F)
95 J @ -20°C,
(70 ft-lb @ -20 °F)
75 J @ -30°C,
(56 ft-lb @ -30 °F)
65 J @ -40°C,
(48 ft-lb @ -40 °F)
125 J @ 0°C,
(93 ft-lb @ 32 °F)
95 J @ -20°C,
(70 ft-lb @ -4 °F)
75 J @ -30°C,
(56 ft-lb @ -22 °F)
30 %
OK Autrod 12.10 Po svaření EN AC 385 MPa 470 MPa
(68 ksi)
150 J @ 0°C,
(111 ft-lb @ 32 °F)
120 J @ -20°C,
(89 ft-lb @ -4 °F)
85 J @ -30°C,
(63 ft-lb @ -22 °F)
70 J @ -40°C,
(52 ft-lb @ -40 °F)
30 %
OK Autrod 12.20 Po svaření AWS DC+ 410 MPa
(59 ksi)
510 MPa
(74 ksi)
135 J @ 20°C,
(100 ft-lb @ 20 °F)
125 J @ 0°C,
(93 ft-lb @ 0 °F)
80 J @ -20°C,
(59 ft-lb @ -20 °F)
55 J @ -40°C,
(41 ft-lb @ -40 °F)
135 J @ 20°C,
(100 ft-lb @ 68 °F)
125 J @ 0°C,
(93 ft-lb @ 32 °F)
80 J @ -20°C,
(59 ft-lb @ -4 °F)
29 %
OK Autrod 12.20 Po svaření EN AC 430 MPa 535 MPa
(78 ksi)
150 J @ 20°C,
(111 ft-lb @ 68 °F)
130 J @ 0°C,
(96 ft-lb @ 32 °F)
115 J @ -20°C,
(85 ft-lb @ -4 °F)
70 J @ -40°C,
(52 ft-lb @ -40 °F)
33 %
OK Autrod 12.22 Po svaření AWS DC+ 425 MPa
(62 ksi)
520 MPa
(75 ksi)
140 J @ 0°C,
(104 ft-lb @ 0 °F)
100 J @ -20°C,
(74 ft-lb @ -20 °F)
60 J @ -40°C,
(44 ft-lb @ -40 °F)
40 J @ -46°C,
(30 ft-lb @ -46 °F)
140 J @ 0°C,
(104 ft-lb @ 32 °F)
100 J @ -20°C,
(74 ft-lb @ -4 °F)
40 J @ -46°C,
(30 ft-lb @ -50.8 °F)
29 %
OK Autrod 12.22 Po svaření EN AC 460 MPa 550 MPa
(80 ksi)
145 J @ 0°C,
(107 ft-lb @ 32 °F)
125 J @ -20°C,
(93 ft-lb @ -4 °F)
90 J @ -40°C,
(67 ft-lb @ -40 °F)
28 %
OK Autrod 12.22L PWHT DC+ 390 MPa
(57 ksi),360 MPa
(52 ksi)
490 MPa
(71 ksi),480 MPa
(70 ksi)
90 J @ -18°C,
(67 ft-lb @ -0.4 °F)
65 J @ -29°C,
(48 ft-lb @ -20.2 °F)
40 J @ -40°C,
(30 ft-lb @ -40 °F)
30 J @ -46°C,
(22 ft-lb @ -50.8 °F)
60 J @ -29°C,
(44 ft-lb @ -20.2 °F)
100 J @ -29°C,
(74 ft-lb @ -20.2 °F)
32 %,36 %,33 % 1 hr,6 hr,10 hr
OK Autrod 12.22L Po svaření DC+ 450 MPa
(65 ksi)
540 MPa
(78 ksi)
60 J @ -18°C,
(44 ft-lb @ -0.4 °F)
45 J @ -29°C,
(33 ft-lb @ -20.2 °F)
30 J @ -40°C,
(22 ft-lb @ -40 °F)
29 %
OK Autrod 12.24 Po svaření AWS DC+ 500 MPa
(73 ksi)
580 MPa
(84 ksi)
125 J @ 20°C,
(93 ft-lb @ 20 °F)
100 J @ 0°C,
(74 ft-lb @ 0 °F)
60 J @ -18°C,
(44 ft-lb @ -18 °F)
40 J @ -29°C,
(30 ft-lb @ -29 °F)
125 J @ 20°C,
(93 ft-lb @ 68 °F)
100 J @ 0°C,
(74 ft-lb @ 32 °F)
60 J @ -18°C,
(44 ft-lb @ -0.4 °F)
40 J @ -29°C,
(30 ft-lb @ -20.2 °F)
24 %
OK Autrod 12.24 Po svaření EN AC 550 MPa 620 MPa
(90 ksi)
130 J @ 20°C,
(96 ft-lb @ 68 °F)
110 J @ 0°C,
(81 ft-lb @ 32 °F)
70 J @ -20°C,
(52 ft-lb @ -4 °F)
40 J @ -40°C,
(30 ft-lb @ -40 °F)
23 %
OK Autrod 12.24L PWHT DC+ 480 MPa
(70 ksi)
560 MPa
(81 ksi)
80 J @ 0°C,
(59 ft-lb @ 32 °F)
50 J @ -18°C,
(37 ft-lb @ -0.4 °F)
26 % 1 hr
OK Autrod 12.24L Po svaření DC+ 550 MPa
(80 ksi)
610 MPa
(88 ksi)
90 J @ 0°C,
(67 ft-lb @ 32 °F)
65 J @ -18°C,
(48 ft-lb @ -0.4 °F)
40 J @ -29°C,
(30 ft-lb @ -20.2 °F)
23 %
OK Autrod 12.30 Po svaření EN AC 510 MPa 590 MPa
(86 ksi)
140 J @ 20°C,
(104 ft-lb @ 68 °F)
120 J @ 0°C,
(89 ft-lb @ 32 °F)
100 J @ -20°C,
(74 ft-lb @ -4 °F)
70 J @ -30°C,
(52 ft-lb @ -22 °F)
28 %
OK Autrod 12.30 Po svaření EN DC+ 490 MPa 580 MPa
(84 ksi)
130 J @ 20°C,
(96 ft-lb @ 20 °F)
110 J @ 0°C,
(81 ft-lb @ 0 °F)
90 J @ -20°C,
(67 ft-lb @ -20 °F)
60 J @ -30°C,
(44 ft-lb @ -30 °F)
130 J @ 20°C,
(96 ft-lb @ 68 °F)
110 J @ 0°C,
(81 ft-lb @ 32 °F)
90 J @ -20°C,
(67 ft-lb @ -4 °F)
60 J @ -30°C,
(44 ft-lb @ -22 °F)
29 %
OK Autrod 12.32 Po svaření AWS DC+ 480 MPa
(70 ksi)
580 MPa
(84 ksi)
150 J @ 20°C,
(111 ft-lb @ 20 °F)
130 J @ 0°C,
(96 ft-lb @ 0 °F)
95 J @ -20°C,
(70 ft-lb @ -20 °F)
65 J @ -40°C,
(48 ft-lb @ -40 °F)
40 J @ -46°C,
(30 ft-lb @ -46 °F)
150 J @ 20°C,
(111 ft-lb @ 68 °F)
130 J @ 0°C,
(96 ft-lb @ 32 °F)
95 J @ -20°C,
(70 ft-lb @ -4 °F)
40 J @ -46°C,
(30 ft-lb @ -50.8 °F)
28 %
OK Autrod 12.32 Po svaření EN AC 530 MPa 615 MPa
(89 ksi)
140 J @ 20°C,
(104 ft-lb @ 68 °F)
120 J @ 0°C,
(89 ft-lb @ 32 °F)
100 J @ -20°C,
(74 ft-lb @ -4 °F)
60 J @ -40°C,
(44 ft-lb @ -40 °F)
28 %
OK Autrod 12.33L PWHT DC+ 550 MPa
(80 ksi)
650 MPa
(94 ksi)
70 J @ 0°C,
(52 ft-lb @ 32 °F)
40 J @ -18°C,
(30 ft-lb @ -0.4 °F)
30 % 1 hr
OK Autrod 12.33L Po svaření DC+ 630 MPa
(91 ksi)
700 MPa
(102 ksi)
65 J @ 0°C,
(48 ft-lb @ 32 °F)
35 J @ -18°C,
(26 ft-lb @ -0.4 °F)
25 %
OK Autrod 12.34 Po svaření AWS DC+ 535 MPa
(78 ksi)
620 MPa
(90 ksi)
120 J @ 20°C,
(89 ft-lb @ 20 °F)
105 J @ 0°C,
(78 ft-lb @ 0 °F)
70 J @ -20°C,
(52 ft-lb @ -20 °F)
60 J @ -30°C,
(44 ft-lb @ -30 °F)
45 J @ -40°C,
(33 ft-lb @ -40 °F)
120 J @ 20°C,
(89 ft-lb @ 68 °F)
105 J @ 0°C,
(78 ft-lb @ 32 °F)
70 J @ -20°C,
(52 ft-lb @ -4 °F)
60 J @ -30°C,
(44 ft-lb @ -22 °F)
27 %
OK Autrod 12.34 Po svaření EN AC 560 MPa 635 MPa
(92 ksi)
135 J @ 20°C,
(100 ft-lb @ 68 °F)
120 J @ 0°C,
(89 ft-lb @ 32 °F)
100 J @ -20°C,
(74 ft-lb @ -4 °F)
80 J @ -30°C,
(59 ft-lb @ -22 °F)
60 J @ -40°C,
(44 ft-lb @ -40 °F)
23 %
OK Autrod 12.40L PWHT DC+ 440 MPa
(64 ksi)
530 MPa
(77 ksi)
100 J @ -18°C,
(74 ft-lb @ -0.4 °F)
80 J @ -29°C,
(59 ft-lb @ -20.2 °F)
55 J @ -40°C,
(41 ft-lb @ -40 °F)
45 J @ -46°C,
(33 ft-lb @ -50.8 °F)
29 % 1 hr
OK Autrod 12.40L Po svaření DC+ 490 MPa
(71 ksi)
580 MPa
(84 ksi)
75 J @ -18°C,
(56 ft-lb @ -0.4 °F)
60 J @ -29°C,
(44 ft-lb @ -20.2 °F)
40 J @ -40°C,
(30 ft-lb @ -40 °F)
27 %
OK Autrod 13.24 Po svaření AWS DC+ 560 MPa
(81 ksi)
630 MPa
(91 ksi)
120 J @ 20°C,
(89 ft-lb @ 20 °F)
85 J @ -20°C,
(63 ft-lb @ -20 °F)
70 J @ -30°C,
(52 ft-lb @ -30 °F)
60 J @ -40°C,
(44 ft-lb @ -40 °F)
40 J @ -46°C,
(30 ft-lb @ -46 °F)
120 J @ 20°C,
(89 ft-lb @ 68 °F)
85 J @ -20°C,
(63 ft-lb @ -4 °F)
70 J @ -30°C,
(52 ft-lb @ -22 °F)
40 J @ -46°C,
(30 ft-lb @ -50.8 °F)
25 %
OK Autrod 13.24 Po svaření EN AC 610 MPa 680 MPa
(99 ksi)
150 J @ 20°C,
(111 ft-lb @ 68 °F)
120 J @ -20°C,
(89 ft-lb @ -4 °F)
100 J @ -30°C,
(74 ft-lb @ -22 °F)
90 J @ -40°C,
(67 ft-lb @ -40 °F)
25 %
OK Autrod 13.27 Po svaření AWS DC+ 500 MPa
(73 ksi)
600 MPa
(87 ksi)
100 J @ -20°C,
(74 ft-lb @ -20 °F)
60 J @ -40°C,
(44 ft-lb @ -40 °F)
50 J @ -51°C,
(37 ft-lb @ -51 °F)
100 J @ -20°C,
(74 ft-lb @ -4 °F)
50 J @ -51°C,
(37 ft-lb @ -59.8 °F)
28 %
OK Autrod 13.27 Po svaření EN AC 530 MPa 620 MPa
(90 ksi)
120 J @ -20°C,
(89 ft-lb @ -4 °F)
90 J @ -40°C,
(67 ft-lb @ -40 °F)
60 J @ -50°C,
(44 ft-lb @ -58 °F)
28 %
OK Autrod 13.36 Po svaření AWS DC+ 490 MPa
(71 ksi)
580 MPa
(84 ksi)
120 J @ 20°C,
(89 ft-lb @ 20 °F)
70 J @ -20°C,
(52 ft-lb @ -20 °F)
55 J @ -29°C,
(41 ft-lb @ -29 °F)
120 J @ 20°C,
(89 ft-lb @ 68 °F)
70 J @ -20°C,
(52 ft-lb @ -4 °F)
55 J @ -29°C,
(41 ft-lb @ -20.2 °F)
27 %
OK Autrod 13.36 Po svaření EN AC 515 MPa 590 MPa
(86 ksi)
150 J @ 20°C,
(111 ft-lb @ 68 °F)
90 J @ -20°C,
(67 ft-lb @ -4 °F)
80 J @ -30°C,
(59 ft-lb @ -22 °F)
27 %
OK Autrod 13.62 Po svaření (acc. AWS) Plate thickness 12mm; Heat Input 2.2kJ/mm; Side 1 600A, 32V, 53cm/min; Side 2 700A, 60cm/min. DC+ 510 MPa
(74 ksi)
610 MPa
(88 ksi)
40 J @ -51°C,
(30 ft-lb @ -51 °F)
40 J @ -51°C,
(30 ft-lb @ -59.8 °F)
28 %
OK Autrod 13.64 Po svaření (acc. to AWS) Plate thickness 12mm Heat input 2.2kJ/mm 700A, 32V, 60cm/min DC+ 550 MPa
(80 ksi)
650 MPa
(94 ksi)
40 J @ -51°C,
(30 ft-lb @ -51 °F)
40 J @ -51°C,
(30 ft-lb @ -59.8 °F)
28 %

Chemické složení svarového kovu

Typického chemické složení svarového kovu v %
C Cr Cu Mn Mo Ni P S Si
ESAB SA10K DC+ 550A, 29V
0.07 % - - 1.75 % - - - - 0.50 %
OK Autrod 12.08L DC+ 550A, 29V
0.06 % - - 0.90 % - - - - 0.20 %
OK Autrod 12.10 AC , 580A, 29V
0.05 % - - 0.85 % - - - - 0.2 %
OK Autrod 12.10 DC+ , 580A, 29V
0.04 % - - 1.0 % - - - - 0.3 %
OK Autrod 12.20 AC, 580A, 29V
0.06 % - - 1.2 % - - - - 0.2 %
OK Autrod 12.20 DC+, 580A, 29V
0.05 % - - 1.35 % - - - - 0.3 %
OK Autrod 12.22 AC, 580A, 29V
0.06 % - - 1.2 % - - - - 0.4 %
OK Autrod 12.22 DC+, 580A, 29V
0.05 % - - 1.4 % - - - - 0.5 %
OK Autrod 12.22L DC+ 550A, 29V
0.08 % - - 1.35 % - - - - 0.40 %
OK Autrod 12.24 AC, 580A, 29V
0.06 % - - 1.3 % 0.5 % - - - 0.25 %
OK Autrod 12.24 DC+, 580A, 29V
0.05 % - - 1.4 % 0.5 % - - - 0.4 %
OK Autrod 12.24L DC+ 550A, 29V
0.08 % - - 1.35 % 0.45 % - 0.025 % 0.020 % 0.40 %
OK Autrod 12.30 AC, 580A, 29V
0.10 % - - 1.6 % - - - - 0.3 %
OK Autrod 12.30 DC+, 580A, 29V
0.09 % - - 1.65 % - - - - 0.4 %
OK Autrod 12.32 AC, 580A, 29V
0.10 % - - 1.9 % - - - - 0.35 %
OK Autrod 12.32 DC+, 580A, 29V
0.09 % - - 2.0 % - - - - 0.5 %
OK Autrod 12.33L DC+
0.06 % - - 1.95 % 0.40 % - - - 0.75 %
OK Autrod 12.34 AC, 580A, 29V
0.10 % - - 1.5 % 0.5 % - - - 0.25 %
OK Autrod 12.34 DC+, 580A, 29V
0.09 % - - 1.6 % 0.5 % - - - 0.4 %
OK Autrod 12.40L DC+ 550A, 29V
0.07 % - - 1.95 % - - - - 0.40 %
OK Autrod 13.24 AC , 580A, 29V
0.09 % - - 1.50 % 0.2 % 0.9 % - - 0.45 %
OK Autrod 13.24 DC+, 580A, 29V
0.07 % - - 1.70 % 0.2 % 0.9 % - - 0.5 %
OK Autrod 13.27 AC, 580A, 29V
0.06 % - - 1.3 % - 2.2 % - - 0.3 %
OK Autrod 13.27 DC+, 580A, 29V
0.05 % - - 1.4 % - 2.2 % - - 0.4 %
OK Autrod 13.36 AC , 580A, 29V
0.09 % 0.3 % 0.5 % 1.2 % - 0.7 % - - 0.4 %
OK Autrod 13.36 DC+, 580A, 29V
0.08 % 0.3 % 0.5 % 1.3 % - 0.7 % - - 0.5 %
x

Objednací číslo a příslušenství

Objednací číslo : OK Flux 10.71
1071H00200 FIND A DISTRIBUTOR
1071000200 FIND A DISTRIBUTOR
1071800P00 FIND A DISTRIBUTOR
1071800P0W FIND A DISTRIBUTOR
1071H02200 FIND A DISTRIBUTOR