Exaton 49S
Exaton 49S is a basic, agglomerated flux for electroslag strip surfacing. This flux is particularly intended for high-speed welding. In spite of high welding speed, flux Exaton 49S gives excellent slag removal and bead appearance, also for niobium-alloyed strip electrodes. It is used together with strip electrodes of the chromium, chromium-nickel and chromium-nickel-molybdenum steel types with or without niobium.
Klasifikace
Jakost | (E) S A FB 2 |
Název | EN ISO 14174 |
Charakteristika svařovacího materiálu
Index bazicity | nom: 4.4 |
Hustota | nom: 1.0 Kg/l |
Typ strusky | Fluoride basic CaF2-Al2O3 |
Svařovací proud | 2200 A (Using 60x0.5 mm strip) |
Klasifikace
Svařovací drát | AWS/EN |
Exaton 19.12.3.L | A5.9:EQ316L/ 14343-A:B 19 12 3 L |
Exaton 19.13.4.L | A5.9:EQ317L/ 14343-A:B 19 13 4 L |
Exaton 19.9.LNb | A5.9:EQ347/ 14343-A:B 19 9 Nb |
Exaton 19.9.L | A5.9:EQ308L/ 14343-A:B 19 9 L |
Exaton 23.11.LNb | A5.9:EQ”309LNb”/ 14343-A:B 23 12 L Nb |
Exaton 24.13.LNb | A5.9:EQ”309LNb”/ 14343-A:B 23 12 Nb |
Exaton 24.13.L | A5.9:EQ309L/ 14343-A:B 23 12 L |
Exaton 21.11.LNb | A5.9:EQ”309LNb”/ 14343-A:B 22 11 L Nb |
Exaton 22.11.L | A5.9:EQ(309L)/ 14343-A:B 22 11 L |
Schválení
Svařovací drát |
*Pouze pro vybraný výrobní závod. Pro další informace prosím kontaktujte ESAB. Navštivte stránky esab.com a stáhněte si materiálový list konkrétní kombinaci tavidlo/drát kde jsou uvedeny potřebné detaily. |
Chemické složení svarového kovu
Typického chemické složení svarového kovu v % | ||||||||||||||
C | Cr | Cu | FN WRC-92 | Mn | Mo | N | Nb | Ni | P | S | Si | Si+Fe | ||
Exaton 19.12.3.L Layer 1 with "24.13.L" | ||||||||||||||
<=0.03 % | 17.7 % | - % | - | - % | 2.2 % | - | - | 12.0 % | - % | - % | - % | 6 % | ||
Exaton 19.13.4.L Layer 1 with "24.13.L" | ||||||||||||||
<=0.03 % | 18.5 % | - % | - | - % | 2.7 % | - | - | 13.0 % | - % | - % | - % | 6 % | ||
Exaton 19.9.L Layer 1 with "24.13.L" | ||||||||||||||
<=0.03 % | 19.2 % | - % | - | - % | - % | - | - | 10 % | - % | - % | - % | 8 % | ||
Exaton 19.9.LNb (Layer 1 with "24.13.L" & Layer 2 with "19.9.LNb") | ||||||||||||||
0.02 % | 19.5 % | - % | - | 1.3 % | 0.1 % | 0.03 % | 0.3 % | 10.6 % | - % | - % | 0.3 % | - % | ||
Exaton 19.9.LNb (Layer 1 with "24.13.LNb" & Layer 2 with "19.9.LNb") | ||||||||||||||
0.02 % | 19.6 % | - % | - | 1.4 % | 0.1 % | 0.03 % | 0.4 % | 10.5 % | - % | - % | 0.3 % | - % | ||
Exaton 21.11.LNb (1 layer) | ||||||||||||||
0.02 % | 18.9 % | - % | - | 1.4 % | 0.1 % | 0.05 % | 0.5 % | 9.7 % | - % | - % | 0.4 % | - % | ||
Exaton 23.11.LNb 1 layer with "23.11.LNb" | ||||||||||||||
<=0.05 % | 19 % | - % | - % | 6.5 % | - % | - % | - | - % | 9.7 % | - % | - % | - % | - | |
Exaton 24.13.L | ||||||||||||||
<=0.07 % | 19 % | - % | - | - % | - % | - | - | 10.2 % | - % | - % | - % | 6 % | ||
Exaton 24.13.LNb | ||||||||||||||
<=0.06 % | 18.5 % | - % | - | - % | - % | - | - % | 9.7 % | - % | - % | - % | 5 % |