Exaton 25.22.2.LMn
Exaton 25.22.2.LMn is a chromium-nickel-molybdenum strip electrode used for electro-slag welding (ESW) or submerged arc welding (SAW) to deposit a second layer corrosion resistant alloy of 25%Cr/22%Ni/2%Mo composition on carbon- and low alloyed steels. It can also be used as buffer layer before depositing second layers.
Klasifikace
Klasifikace |
EN ISO 14343-A : B 25 22 2 N L SFA/AWS A5.9 : EQ"310LMo" |
Chemické složení svarového kovu
Typical Wire Composition % | ||||||||||||||
C | Cr | Mn | Mo | N | Ni | P | S | Si | ||||||
<=0.020 % | 25.0 % | 4.5 % | 2.1 % | 0.13 % | 22.0 % | <=0.015 % | <=0.015 % | <=0.2 % |