Exaton 24.29.5.LCu
Exaton 24.29.5.LCu is a copper alloyed chromium-nickel-molybdenum strip electrode used for electro-slag welding (ESW) or submerged arc welding (SAW). In ESW, single layer overlays on carbon- and low alloyed steels of E385 composition can be deposited. In SAW, buffer layers of 20%Cr/25%Ni/5%Mo/Cu composition can be deposited on carbon- and low alloyed steels before surfacing of second layers of 904/385 composition using Exaton 20.25.5.LCu.
Klasifikace
Jakost | EQ(385) |
Název | SFA/AWS A5.9 |
Chemické složení svarového kovu
Typical Wire Composition % | ||||||||||||||
C | Cr | Cu | Mn | Mo | Ni | P | S | Si | ||||||
<=0.020 % | 23.5 % | 1.8 % | 2 % | 5.4 % | 29 % | <=0.015 % | <=0.015 % | 0.4 % |