Exaton 24.13.LNb is a niobium stabilized chromium-nickel strip electrode used for submerged arc welding (SAW) to deposit a buffer layer of stabilized corrosion resistant alloy of 19%Cr/9%Ni composition on carbonand low alloyed steels. In high speed electro-slag welding (ESW) it can be used for single layer deposits of 347 composition on carbon- and low alloyed steels. It can also be combined with 19.9.LNb for surfacing of two layer overlays.

BUY NOW


Klasifikace

Klasifikace SFA/AWS A5.9 : EQ”309LNb”
EN ISO 14343-A : B 23 12 Nb

Chemické složení svarového kovu

Typical Wire Composition %
C Cr Cu Mn Mo Nb Ni P S Si Si+Fe
<=0.02 % 24 % <=0.3 % 2 % <=0.3 % 0.75 % 12.5 % <=0.020 % <=0.020 % 0.3 % 22 %
x

Objednací číslo a příslušenství

Objednací číslo : Exaton 24.13.LNb
S166530200 FIND A DISTRIBUTOR
S16653020P FIND A DISTRIBUTOR
S166560200 FIND A DISTRIBUTOR
S16656020P FIND A DISTRIBUTOR
S166560500 FIND A DISTRIBUTOR
S16656050P FIND A DISTRIBUTOR
S166590X00 FIND A DISTRIBUTOR
S166591000 FIND A DISTRIBUTOR
S16659020P FIND A DISTRIBUTOR
S16659080P FIND A DISTRIBUTOR
S166590Y00 FIND A DISTRIBUTOR
x
x

x

Loading..