Exaton 23.11.LNb
Exaton 23.11.LNb is a niobium stabilized chromium-nickel strip electrode particularly suited for high speed electro-slag welding (ESW) to deposit a single layer overlay of stabilized corrosion resistant alloy of 19%Cr/9%Ni composition on carbon- and low alloyed steels. It can also be combined with 19.9.LNb for surfacing of two layer overlays.
Klasifikace
Klasifikace |
EN ISO 14343-A : B 23 12 L Nb SFA/AWS A5.9 : EQ”309LNb” |
Chemické složení svarového kovu
Typical Wire Composition % | ||||||||||||||
C | Cr | Cu | FN WRC-92 | Mn | Mo | Nb | Ni | P | S | Si | ||||
<=0.02 % | 23 % | <=0.2 % | - % | 2.0 % | <=0.2 % | 0.75 % | 12 % | <=0.020 % | <=0.015 % | 0.2 % |