Exaton 22.11.L
Exaton 22.11.L is a chromium-nickel strip electrode used for electro-slag welding (ESW) to deposit a single layer overlay of corrosion resistant alloy of 19%Cr/9%Ni composition on carbon- and low alloyed steels. It can also be combined with 19.9.L for surfacing of two layer overlays.
Klasifikace
Klasifikace |
EN ISO 14343-A : B 22 11 L SFA/AWS A5.9 : EQ(309L) |
Chemické složení svarového kovu
Typical Wire Composition % | ||||||||||||||
C | Cr | Cu | Mn | Mo | Ni | P | S | Si | Si+Fe | |||||
<=0.015 % | 21 % | <=0.1 % | 1.8 % | <=0.3 % | 11.5 % | <=0.020 % | <=0.020 % | 0.2 % | 13 % |