Exaton 21.11.LNb
Exaton 21.11.LNb is a niobium stabilized chromium-nickel strip electrode used for electro-slag welding (ESW) to deposit a single layer overlay of stabilized corrosion resistant alloy of 19%Cr/9%Ni composition on carbon and low alloyed steels. It can also be combined with 19.9.LNb for surfacing of two layer overlays.
Klasifikace
Klasifikace |
SFA/AWS A5.9 : EQ”309LNb” EN ISO 14343-A : B 22 11 L Nb |
Chemické složení svarového kovu
Typical Wire Composition % | ||||||||||||||
C | Cr | Cu | Mn | Mo | N | Nb | Ni | P | S | Si | Si+Fe | |||
<=0.015 % | 21 % | <=0.3 % | 1.8 % | <=0.3 % | - % | 0.55 % | 11 % | <=0.020 % | <=0.020 % | 0.2 % | 14 % |