Exaton 19.9.LNb is a niobium stabilized chromium-nickel strip electrode used for electro-slag welding (ESW) or submerged arc welding (SAW) to deposit a second layer corrosion resistant alloy of stabilized 19%Cr/9%Ni composition on carbon- and low alloyed steels. The buffer layer is deposited using an over-alloyed consumable, such as 21.11.LNb or 24.13.LNb.

BUY NOW


Klasifikace

Klasifikace EN ISO 14343-A : B 19 9 Nb
SFA/AWS A5.9 : EQ347

Chemické složení svarového kovu

Typical Wire Composition %
C Cr Cu Mn Mo N Nb Ni P S Si Si+Fe
<=0.02 % 20 % <=0.3 % 1.8 % <=0.3 % - % 0.5 % 10.5 % <=0.02 % <=0.02 % 0.4 % 11 %
x

Objednací číslo a příslušenství

Objednací číslo : Exaton 19.9.LNb
S162510W00 FIND A DISTRIBUTOR
S162520200 FIND A DISTRIBUTOR
S162530200 FIND A DISTRIBUTOR
S16253020P FIND A DISTRIBUTOR
S162540200 FIND A DISTRIBUTOR
S162450200 FIND A DISTRIBUTOR
S162550200 FIND A DISTRIBUTOR
S162560200 FIND A DISTRIBUTOR
S16256020P FIND A DISTRIBUTOR
S162560500 FIND A DISTRIBUTOR
S16256050P FIND A DISTRIBUTOR
S162480200 FIND A DISTRIBUTOR
S162591000 FIND A DISTRIBUTOR
S16259020P FIND A DISTRIBUTOR
S162590200 FIND A DISTRIBUTOR
S16259080P FIND A DISTRIBUTOR
x
x

x

Loading..