Exaton 19.13.4.L
Exaton 19.13.4.L is a chromium-nickel-molybdenum strip electrode used for electro-slag welding (ESW) or submerged arc welding (SAW) to deposit a second layer corrosion resistant alloy of 19%Cr/13%Ni/4%Mo composition on carbon- and low alloyed steels. The buffer layer is deposited using an over-alloyed consumable, such as 21.13.3.L, 22.11.L or 24.13.L
Klasifikace
Klasifikace |
SFA/AWS A5.9 : EQ317L EN ISO 14343-A : B 19 13 4 L |
Chemické složení svarového kovu
Typical Wire Composition % | ||||||||||||||
C | Cr | Cu | Mn | Mo | Ni | P | S | Si | Si+Fe | |||||
<=0.02 % | 19 % | <=0.3 % | 1.5 % | 3.6 % | 14 % | <=0.020 % | <=0.020 % | 0.4 % | 7 % |