Unfortunately metal markets continue to force us to take the regrettable action of applying alloy surcharges. The surcharge will affect stainless and nickel steel filler metal products, namely covered electrodes, bare and cored wires. These rates will change monthly as market prices continue to vary. We understand the difficulty that raw material surcharges cause for our valued customers, however we feel this is the fairest way to deal with these extraordinary fluctuations in raw materials. Your continued cooperation and understanding is appreciated. Contact your local ESAB Territory Sales Manager for additional information.
For more information about alloy surcharges, please vist the London Metal Exchange's website.
Regards,
Marketing Department
Filler Metal Welding Consumables
| Stainless Steel Alloy | 05/05/2008 |
|---|---|
| 307 | $1.86 |
| 308, 308L, 308LSi, 308H | $2.40 |
| 309, 309L, 309LSi, 309LMo, 309Nb | $3.10 |
| 310, 310Mo, 310Cb | $3.56 |
| 312 | $2.06 |
| 316, 316L, 316LSi, 316H | $3.43 |
| 317, 317L | $3.66 |
| 320, 320LR | $5.36 |
| 347, 347H | $2.40 |
| 2209, 2509 | $3.14 |
| 410 | $0.53 |
| 410NiMo | $1.30 |
| 409Ti, 409Cb | $0.15 |
| 430LCb, 439Ti, 18CrCb | $0.20 |
| Nickel Alloy (covered electrode & cored wire) | |
| Nickel-Arc 55 & 550, Nicore 55, All-State 4-60, Super 4-60, 8-60, Corecast 8600 | $5.74 |
| Nickel-Arc 99, All-State 4IMP, #8 & Nickel NC | $9.56 |
| Arcaloy 112 & ENiCrMo-3 | $9.38 |
| ENiCrMo-6 | $10.46 |
| Arcaloy 8N12 | $7.42 |
| Arcaloy 9N10 | $7.82 |
| Arcaloy 276 | $10.70 |
| Nickel Alloy (solid bare wire) | |
| Nickel 55, All-State 4-60T | $7.26 |
| Nickel 99, All-State 4-T | $12.80 |
| Arcaloy 276 | $13.50 |
| Arcaloy 82 | $9.90 |
| Arcaloy 625 | $11.80 |
| Stainless Steel Alloy | 04/07/2008 |
|---|---|
| 307 | $1.60 |
| 308, 308L, 308LSi, 308H | $2.08 |
| 309, 309L, 309LSi, 309LMo, 309Nb | $2.70 |
| 310, 310Mo, 310Cb | $3.10 |
| 312 | $1.80 |
| 316, 316L, 316LSi, 316H | $3.08 |
| 317, 317L | $3.32 |
| 320, 320LR | $4.76 |
| 347, 347H | $2.08 |
| 2209, 2509 | $2.86 |
| 410 | $0.46 |
| 410NiMo | $1.16 |
| 409Ti, 409Cb | $0.15 |
| 430LCb, 439Ti, 18CrCb | $0.20 |
| Nickel Alloy (covered electrode & cored wire) | |
| Nickel-Arc 55 & 550, Nicore 55, All-State 4-60, Super 4-60, 8-60, Corecast 8600 | $4.94 |
| Nickel-Arc 99, All-State 4IMP, #8 & Nickel NC | $8.24 |
| Arcaloy 112 & ENiCrMo-3 | $8.40 |
| ENiCrMo-6 | $10.24 |
| Arcaloy 8N12 | $6.40 |
| Arcaloy 9N10 | $6.78 |
| Arcaloy 276 | $9.80 |
| Nickel Alloy (solid bare wire) | |
| Nickel 55, All-State 4-60T | $6.24 |
| Nickel 99, All-State 4-T | $10.98 |
| Arcaloy 276 | $12.34 |
| Arcaloy 82 | $8.50 |
| Arcaloy 625 | $10.56 |
| Stainless Steel Alloy | 03/03/2008 |
|---|---|
| 307 | $1.58 |
| 308, 308L, 308LSi, 308H | $1.96 |
| 309, 309L, 309LSi, 309LMo, 309Nb | $2.58 |
| 310, 310Mo, 310Cb | $3.00 |
| 312 | $1.70 |
| 316, 316L, 316LSi, 316H | $2.98 |
| 317, 317L | $3.28 |
| 320, 320LR | $4.60 |
| 347, 347H | $1.96 |
| 2209, 2509 | $2.80 |
| 410 | $0.40 |
| 410NiMo | $1.12 |
| 409Ti, 409Cb | $0.15 |
| 430LCb, 439Ti, 18CrCb | $0.20 |
| Nickel Alloy (covered electrode & cored wire) | |
| Nickel-Arc 55 & 550, Nicore 55, All-State 4-60, Super 4-60, 8-60, Corecast 8600 | $4.84 |
| Nickel-Arc 99, All-State 4IMP, #8 & Nickel NC | $8.10 |
| Arcaloy 112 & ENiCrMo-3 | $8.20 |
| ENiCrMo-6 | $9.90 |
| Arcaloy 8N12 | $6.28 |
| Arcaloy 9N10 | $6.60 |
| Arcaloy 276 | $9.60 |
| Nickel Alloy (solid bare wire) | |
| Nickel 55, All-State 4-60T | $6.16 |
| Nickel 99, All-State 4-T | $10.84 |
| Arcaloy 276 | $12.10 |
| Arcaloy 82 | $8.36 |
| Arcaloy 625 | $10.34 |
| Stainless Steel Alloy | 02/04/2008 |
|---|---|
| 307 | $1.52 |
| 308, 308L, 308LSi, 308H | $1.82 |
| 309, 309L, 309LSi, 309LMo, 309Nb | $2.40 |
| 310, 310Mo, 310Cb | $2.82 |
| 312 | $1.60 |
| 316, 316L, 316LSi, 316H | $2.84 |
| 317, 317L | $3.12 |
| 320, 320LR | $4.34 |
| 347, 347H | $1.82 |
| 2209, 2509 | $2.68 |
| 410 | $.38 |
| 410NiMo | $1.08 |
| 409Ti, 409Cb | $0.15 |
| 430LCb, 439Ti, 18CrCb | $0.20 |
| Nickel Alloy (covered electrode & cored wire) | |
| Nickel-Arc 55 & 550, Nicore 55, All-State 4-60, Super 4-60, 8-60, Corecast 8600 | $4.42 |
| Nickel-Arc 99, All-State 4IMP, #8 & Nickel NC | $7.44 |
| Arcaloy 112 & ENiCrMo-3 | $7.68 |
| ENiCrMo-6 | $9.31 |
| Arcaloy 8N12 | $5.74 |
| Arcaloy 9N10 | $6.02 |
| Arcaloy 276 | $9.12 |
| Nickel Alloy (solid bare wire) | |
| Nickel 55, All-State 4-60T | $5.62 |
| Nickel 99, All-State 4-T | $9.94 |
| Arcaloy 276 | $11.50 |
| Arcaloy 82 | $7.64 |
| Arcaloy 625 | $9.70 |