Wear-Arc Hardfacing & Build-up Electrodes

Wear-Arc covered electrodes are uniquely designed for hard-surfacing and build-up. These electrodes provide maximum resistance to specific destructive wear factors such as abrasion, compression, deformation, heat or corrosion.

WEAR-ARC® 4 IP

Wear-Arc 4-IP is an all position, iron powder, low hydrogen hardsurfacing electrode providing sound overlays on carbon and low alloy steels, as well as many abrasion-resistant steels.

WEAR-ARC® 40

Wear-Arc 40 is a coated electrode with a special core wire and the proper amount of alloys in the coating to produce a deposit of highly abrasive resistant chrome carbides in a matrix of iron and chromium.

WEAR-ARC® 6 IP

The iron powder low hydrogen coating of Wear-Arc 6-IP electrodes promotes good bonds with manganese and carbon steels.