All-State SUPER 4-60
Unique AC/DC straight or reverse electrode for heavy sections of cast iron, ductile iron and dissimilar metals. Strong, machinable,crack resistant deposits without porosity, yet spatter free. No overheating at rated amperage. ... [Read more]