Arcair

Arcair Underwater Cutting Electrodes

Arcair Underwater Cutting Electrodes

Arc Gouging Consumables

Model Amperage Capacity Current Type Operating Polarity
Arcwater (42059006) 375 to 400 A DC DCEP (Direct Current Electrode Positive) - Reverse Polarity
Sea-Cut (42059007) Up to 400 A DC DCEP (Direct Current Electrode Positive) - Reverse Polarity
Sea-Dragon (42075005) 1 to 400 A DC DCEP (Direct Current Electrode Positive) - Reverse Polarity
Sea-Jet (42066006) 0 to 400 A DC DCEP (Direct Current Electrode Positive) - Reverse Polarity
Tuff-Cote (42058008) Up to 350 A DC DCEP (Direct Current Electrode Positive) - Reverse Polarity

Dimensions

Diameter Description or Qualifier Length
3/8 in.
9.5 mm
42066006 18 in.
457 mm
3/8 in.
9.5 mm
42075005 18 in.
457 mm
5/16 in.
7.9 mm
42059007 14 in.
355.6 mm
5/16 in.
7.9 mm
42058008 14 in.
355.6 mm
5/16 in.
7.9 mm
42059006 8 in.
229 mm
x
×