Previous Next

Arcair

Professional K-5

Arc Gouging Consumables

Model Amperage Capacity
01104003 Up to 1250 A
61104007 Up to 1250 A
61104008 Up to 1250 A
70128507 Up to 1250 A
70128510 Up to 1250 A

Arc Gouging Specs

Model Air Requirement Amperage Capacity Carbon Electrode Range Conditional Statement Flow Rate
01104003 80 psi
5.6
450-1250 A 30 cfh
850 l/min
01104003 5/16-1/2 in.
7.9-12.7 mm
Pointed
01104003 5/16-5/8 in.
7.9-15.9 mm
Jointed
01104003 5/8 in.
15.9 mm
Half Round
61104007 80 psi
5.6
450-1250 A 30 cfh
850 l/min
61104007 5/16-1/2 in.
7.9-12.7 mm
Pointed
61104007 5/16-5/8 in.
7.9-15.9 mm
Jointed
61104007 5/8 in.
15.9 mm
Half Round
61104008 80 psi
5.6
450-1250 A 30 cfh
850 l/min
61104008 5/16-1/2 in.
7.9-12.7 mm
Pointed
61104008 5/16-5/8 in.
7.9-15.9 mm
Jointed
61104008 5/8 in.
15.9 mm
Half Round