Arcair

CutSkill Gouging Electrodes

CutSkill Gouging Electrodes

General purpose electrodes without the copper plating to avoid any chance of copper contamination in the base material. Same high quality blend of carbon and graphite used in other Arcair electrodes.

Where To Buy


Features

Designed specifically for the air carbon-arc process

  • Contain a precise formulated blend of carbon and graphite
  • Produces the most efficient metal removal performance in today’s market
  • Superior metal removal rates, cool operation, and uniform diameters
Ideal for a broad range of applications
  • Creating u-grooves for weld joint
  • Removing old welds
  • Gouging out cracks
  • Cleaning and repairing castings
  • Removing hard surface material
  • Rough machining