Previous Next

Arcair

CutSkill Angle-Arc CSK4000

Arc Gouging Consumables

Amperage Capacity Up to 1000 A

Arc Gouging Specs

Model Air Requirement Amperage Capacity Carbon Electrode Range Conditional Statement Flow Rate
01088000 80 psig
5.6
1000 A 28 cfh
790 l/min
01088000 5/32-1/2 in.
4.0-12.7 mm
Pointed
01088000 5/16-1/2 in.
7.9-12.7 mm
Jointed
01088000 3/8 and 5/8 in.
9.5-15.9 mm
Flat
01088000 5/8 in.
15.9 mm
Half Round
61088007 5/32-1/2 in.
4.0-12.7 mm
Pointed
61088007 5/16-1/2 in.
7.9-12.7 mm
Jointed
61088007 3/8 and 5/8 in.
9.5-15.9 mm
Flat
61088007 5/8 in.
15.9 mm
Half Round
61088010 5/32-1/2 in.
4.0-12.7 mm
Pointed
61088010 5/16-1/2 in.
7.9-12.7 mm
Jointed
61088010 3/8 and 5/8 in.
9.5-15.9 mm
Flat
61088010 5/8 in.
15.9 mm
Half Round
70088007 5/32-1/2 in.
4.0-12.7 mm
Pointed
70088007 5/16-1/2 in.
7.9-12.7 mm
Jointed
70088007 3/8 and 5/8 in.
9.5-15.9 mm
Flat
70088007 5/8 in.
15.9 mm
Half Round
70088010 5/32-1/2 in.
4.0-12.7 mm
Pointed
70088010 5/16-1/2 in.
7.9-12.7 mm
Jointed
70088010 3/8 and 5/8 in.
9.5-15.9 mm
Flat
70088010 5/8 in.
15.9 mm
Half Round

Weight

Torch and Cable

Weight 2.9 kg (6.47 lb)
x
×