Self-Lighting Air Acetylene

Self-Lighting Air Acetylene

Extreme Swirl Technology delivers high heat, super fast, reducing brazing time and fuel consumption. All air acetylene kits include gauge guards and cylinder wrench. Our best line of self-lighting torch kits are available in either valve rear or valve forward configurations. Improved design features quick-disconnect handles and tips, replaceable tips and color coded “O” rings for quick gas identification.

Where To Buy


Features

  • Quick-disconnect Handles and Tips
  • Replacement Tips
  • Color Coded "O" Rings for Quick Gas Identification
  • Included Features
    • Gauge Guards
    • Cylinder Wrench
    • G-4 Handle
    • PL-8A Tip; Soft solders to 4" (90mm) & Silver brazes to 2" (50mm)
    • Instruction Manual


    Industries

    • Hobbyist
    • HVAC
    • Light Fabrication

Specifications

Operating Specifications

PL-5ADLX-MC

Silver Braze 3/4 in. (20 mm)
Soft Solder 1-1/2 in. (40 mm)

PL-5ADLX-B

Silver Braze 3/4 in. (20 mm)
Soft Solder 1-1/2 in. (40 mm)