Type HPP Two Piece Heavy Preheat Propylene Tip

Type HPP Two Piece Heavy Preheat Propylene Tip

Propylene Heavy Preheat Cutting Tips - Type HPP for heavy preheat scrapping, beveling, and other similar applications.

Where To Buy


Features

  • Heavy preheat
  • Scrap and bevel


Industries

  • Industrial and General Fabrication
  • Light Fabrication
  • Repair and Maintenance
  • Structural Steel Fabrication

Specifications

Fuel Specifications

0333-0282

Gas Pressure - Cutting Oxygen 30-35 psig
Gas Pressure - Fuel Gas 3-5 psig
Total Fuel Gas Consumption 22-110 cfh
Total Oxygen Consumption 70-80 cfh
Total Preheat Oxygen Consumption 44-240 cfh

0333-0283

Gas Pressure - Cutting Oxygen 30-35 psig
Gas Pressure - Fuel Gas 3-6 psig
Total Fuel Gas Consumption 22-110 cfh
Total Oxygen Consumption 70-80 cfh
Total Preheat Oxygen Consumption 44-240 cfh

Operating Specifications

0333-0282

Average Kerf Width 0.06 in.
Cutting Speed 18-22 in./min
Metal Thickness 1/2 in.
Tip Size 0 in.

0333-0283

Average Kerf Width 0.08 in.
Cutting Speed 15-20 in./min
Metal Thickness 3/4 in.