Previous Next

Victor

Type 303MP One Piece Propylene Cutting Tip

Type 303MP One Piece Propylene Cutting Tip

Propylene Cutting Tips - Type 303MP for manual or mechanized torch cutting applications

Add to shopping list


Features

  • General purpose
  • Propylene hand and machine torch cutting


Industries

  • Industrial and General Fabrication
  • Light Fabrication
  • Repair and Maintenance
  • Structural Steel Fabrication

Specifications

Fuel Specifications

0330-0187

Gas Pressure - Cutting Oxygen 20-25 psig
Gas Pressure - Fuel Gas 3-5 psig
Total Fuel Gas Consumption 5-7 cfh
Total Oxygen Consumption 22-.26 cfh
Total Preheat Oxygen Consumption 23-108 cfh

0330-0188

Gas Pressure - Cutting Oxygen 25-30 psig
Gas Pressure - Fuel Gas 3-5 psig
Total Fuel Gas Consumption 8-10 cfh
Total Oxygen Consumption 45-55 cfh
Total Preheat Oxygen Consumption 23-108 cfh

Operating Specifications

0330-0187

Average Kerf Width 0.04 in.
Cutting Speed 21-25 in./min
Metal Thickness 1/4 in.
Tip Size 00 in.

0330-0188

Average Kerf Width 0.06 in.
Cutting Speed 20-24 in./min
Metal Thickness 3/8 in.
Tip Size 0 in.