Type GPN - Two Piece Propane/Natural Gas Cutting Tip

Type GPN - Two Piece Propane/Natural Gas Cutting Tip

LP Cutting Tips - Type GPN for manual and machine cutting applications

Where To Buy


Features

  • General purpose for Propane/Natural Gas applications
  • Two piece hand and machine torch cutting


Industries

  • Industrial and General Fabrication
  • Light Fabrication
  • Repair and Maintenance
  • Structural Steel Fabrication

Specifications

Fuel Specifications

0333-0300

Gas Pressure - Cutting Oxygen 20-25 psig
Gas Pressure - Fuel Gas 3-5 psig
Total Fuel Gas Consumption 5-6 cfh
Total Oxygen Consumption 12-14 cfh
Total Preheat Oxygen Consumption 23-108 cfh

0333-0301

Gas Pressure - Cutting Oxygen 20-25 psig
Gas Pressure - Fuel Gas 3-5 psig
Total Fuel Gas Consumption 5-7 cfh
Total Oxygen Consumption 22-.26 cfh
Total Preheat Oxygen Consumption 23-108 cfh

Operating Specifications

0333-0300

Average Kerf Width 0.04 in.
Cutting Speed 24-28 in./min
Metal Thickness 1/8 in.
Tip Size 000 in.

0333-0301

Average Kerf Width 0.04 in.
Cutting Speed 21-25 in./min
Metal Thickness 1/4 in.
Tip Size 00 in.