Type MTHN High Speed Propane/Natural Gas Cutting Tip

Type MTHN High Speed Propane/Natural Gas Cutting Tip

LP High Speed Machine Cutting Tips - Type MTHN for high speed machine cutting through 10" (252 mm)

Add to shopping list


Features

  • High speed machine cutting through 10" (252 mm)

Industries

  • Industrial and General Fabrication
  • Light Fabrication
  • Repair and Maintenance
  • Structural Steel Fabrication

Specifications

Fuel Specifications

0333-0363

Gas Pressure - Cutting Oxygen 85-95 psig
Gas Pressure - Fuel Gas 8 oz + psig
Gas Pressure - Preheat Oxygen 30-35 psig
Total Fuel Gas Consumption 12-65 cfh
Total Oxygen Consumption 68-75 cfh
Total Preheat Oxygen Consumption 23-140 cfh

0333-0364

Gas Pressure - Cutting Oxygen 85-95 psig
Gas Pressure - Fuel Gas 8 oz + psig
Gas Pressure - Preheat Oxygen 30-35 psig
Total Fuel Gas Consumption 12-65 cfh
Total Oxygen Consumption 110-120 cfh
Total Preheat Oxygen Consumption 23-140 cfh

Operating Specifications

0333-0363

Average Kerf Width 0.05 in.
Cutting Speed 23-30 in./min
Metal Thickness 1/4 in.
Tip Size 00 in.
Average Kerf Width 0.05 in.
Cutting Speed 22-29 in./min
Metal Thickness 3/8 in.
Tip Size 00 in.